ABSTRACT
  In this study, a series of fatigue test was performed to evaluate the fatigue strength of butt welded specimens. Effective notch stress through finite element analysis was conducted to analyze the fatigue results. As a results, no significant decrease in fatigue strength was observed when backplates were present. The S-N curve that based on effective notch stress appeared a similar fatigue life to FAT 225 curve without reference to existence of backplates.
Keywords: Backplate;Fatigue assessment;Butt weld;Effective notch stress
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,011
View
0
Download
Related articles
Studies on the Improvement of Butt Welding Characteristic of Polyethylene Pipes  2011 February;29(1)
Fatigue Properties of Friction Weld According to the Location of Small Artifical Defect   2001 December;19(6)
Fatigue Assessment of Ship Structures : Recent State of the Art   1998 October;16(5)
Studies on the Improvement of Butt Welding Characteristic of Polyethylene Pipes  2011 February;29(1)
Fatigue Properties of Friction Weld According to the Location of Small Artifical Defect   2001 December;19(6)
Fatigue Assessment of Ship Structures : Recent State of the Art   1998 October;16(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.