Microstructure and Mechanical Properties of Clad(A4045/A3003) Al Alloy by Gas Tungsten Arc Welding
Ki-Bin Kim, Jin-Seon Gook, Dong-Ju Yoon, Byung-Il Kim, Il-Cheon Lee




Correspondence:   Published online September 24, 2008
ABSTRACT
  In this paper, research was the variation of microstructure and mechanical properties of clad(A4045/A3003) Al alloy sheet by gas tungsten arc welding. Tensile properties of the gas tungsten arc welding joint decreased because of the softened heat affected zone(HAZ). The hardness of HAZ was lower than that of base metal, because relieved the work hardening effect of the welding heat. Hardness distribution of the weld zone with the base metal appears similarly, but the hardness of HAZ decreased remarkably. The microstructure in the weld zone of A4045 clad layer was formed a coarse columner grains of Si-rich. In the case of large weld heat input, the Si of the A4045 were diffused and until A3003 weld zone they decreased the strength.
Keywords: TIG welding;Clad(A4045/A3003) Al alloy;HAZ;Work hardening;Columner grains
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,413
View
0
Download
Related articles
Microstructure and Mechanical Properties of Friction-Welded Alloy 718 and SNCRW Stainless Steel After Post-Weld Heat-Treatment  2019 August;37(4)
Manufacturing Process of Titanium Alloys Flux-Metal Cored Wire for Gas Tungsten Arc Welding  2019 June;37(3)
Analysis of Microstructure and Mechanical Properties of Friction Stir Vibration Welded (FSVW) 5083 Aluminum Alloy Joints: Experimental and Simulation  2019 June;37(3)
Microstructure and Mechanical Properties in the Friction Stir Welded C70600 Alloy  2018 April;36(2)
Microstructure and Mechanical Properties of Reheated Zones in the Multi-pass Weld Metal of High-Strength Steel  2017 December;35(6)
Microstructure and Mechanical Properties of Friction-Welded Alloy 718 and SNCRW Stainless Steel After Post-Weld Heat-Treatment  2019 August;37(4)
Manufacturing Process of Titanium Alloys Flux-Metal Cored Wire for Gas Tungsten Arc Welding  2019 June;37(3)
Analysis of Microstructure and Mechanical Properties of Friction Stir Vibration Welded (FSVW) 5083 Aluminum Alloy Joints: Experimental and Simulation  2019 June;37(3)
Microstructure and Mechanical Properties in the Friction Stir Welded C70600 Alloy  2018 April;36(2)
Microstructure and Mechanical Properties of Reheated Zones in the Multi-pass Weld Metal of High-Strength Steel  2017 December;35(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.