A Study on Improvement of Fatigue Strength of Electrical Panel Weldments in Naval Vessels by Post Weld Treatment
Myung-Hyun Kim, Min-Su Kang, Sung-Won Kang


Correspondence:   Published online September 24, 2008
ABSTRACT
  Structural reliability of electrical panels installed in naval vessels is of critical importance from structural performance viewpoint. The panels may be exposed to vibration and fatigue loadings from internal and external sources and wave loading which cause fatigue cracking. In this study, common methods such as burr grinding and post weld heat treatment (PWHT), for the fatigue strength improvement of weldments are investigated. Burr grinding is carried out using a electric grinder in order to remove surface defects and improve the weld bead profile. And also PWHT is carried out for the purpose of removing residual. The effectiveness of the two post treatment methods is evaluated in terms of fatigue strength improvement of welded structures.
Keywords: Fatigue;Electrical Panel;PWHT;Burr grinding
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
781
View
0
Download
Related articles
A Study on the Evaluation of Fatigue Strength of Welded Lap Joint with Element Stress Approach  2014 February;32(1)
The Study of Measurement of Residual Stress for Pipe Weldments of Power Plant  2012 April;30(2)
A Study on the Fatigue Strength Improvement using Weld Toe Burr Grinding  2006 April;24(2)
Estimation of Fatigue Strength in Resistance Spot Weldment of the Vehicle Body   2002 April;20(2)
Quality Improvement on Joints of Electronic Materials and Its Reliabilty by Fe-Ni Alloy Clad Lead Frame.   1995 June;13(2)
A Study on the Evaluation of Fatigue Strength of Welded Lap Joint with Element Stress Approach  2014 February;32(1)
The Study of Measurement of Residual Stress for Pipe Weldments of Power Plant  2012 April;30(2)
A Study on the Fatigue Strength Improvement using Weld Toe Burr Grinding  2006 April;24(2)
Estimation of Fatigue Strength in Resistance Spot Weldment of the Vehicle Body   2002 April;20(2)
Quality Improvement on Joints of Electronic Materials and Its Reliabilty by Fe-Ni Alloy Clad Lead Frame.   1995 June;13(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.