A Study on the Effect of Overlap Rate on Laser Beam Cleaning Characteristics while Cleaning Paint Using a Low Power Pulsed Laser(Ⅰ) - Analysis of Laser Cleaned Surface Characteristics Based on Number of Scans -
Ji-Eon Kim1  , Moo-Keun Song2  , Jong-Myoung Lee3  , Jeong-Hun Hyun4  , Jong-Do Kim5 
1Ocean Science and Technology School, Korea Maritime & Ocean Univ., Busan, 49112, Korea
2Laser Advanced Machining Support Center, Korea Maritime & Ocean Univ., Busan, 49112, Korea
3IMT Co., Ltd., Suwon, 16675, Korea
4Daewoo Shipbuilding & Marine Engineering Co., Ltd., Geoje, 53302, Korea
5Division of Marine Engineering, Korea Maritime & Ocean Univ., Busan, 49112, Korea
Correspondence: Jong-Do Kim  Email: jdkim@kmou.ac.kr
Received August 4, 2019  Revised October 8, 2019  Accepted October 14, 2019  Published online October 21, 2019
ABSTRACT
In the shipbuilding and marine fields, the pre-treatment of painted surfaces for cleaning creates environmental pollution problems. Laser cleaning is an eco-friendly surface pre-treatment process which selectively removing contaminants on a surface by vaporizing them with a laser beam. In this study, a pulse laser was employed to laser clean shop primer and epoxy painted steel plates. The evaporation characteristics of the two paints and the laser cleaning characteristics were analyzed according to the number of laser scans. It was determined that the removal of epoxy paint, which has a relatively low evaporation point, was higher than that of the shop primer paint. In addition, to remove the coating surface and oxide layer while minimizing damage to the base metal, it is important to select the laser cleaning parameters including the number of laser scans.
Keywords: Laser cleaning | Pulse laser | Shop primer | Epoxy | The number of laser scans
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
117
View
17
Download
Related article
A Study on the Effect of Overlap Rate on Laser Beam Cleaning Characteristics while Cleaning Paint Using a Low Power Pulsed Laser(Ⅱ) - Analysis of Laser Cleaned Surface Characteristics for Various Pulse Overlap Rates -  2019 October;37(5)
A Study on the Effect of Overlap Rate on Laser Beam Cleaning Characteristics while Cleaning Paint Using a Low Power Pulsed Laser(Ⅱ) - Analysis of Laser Cleaned Surface Characteristics for Various Pulse Overlap Rates -  2019 October;37(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.