P-GMAW에서 용접 자세에 따른 비드 형상 및 재료 물성 변화에 관한 연구
박진형*·김성환*·김노원*·문형순*,†·김명현**,†
*한국생산기술연구원 정밀가공제어그룹
**부산대학교 조선해양공학과
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW
Jin-Hyeong Park*, Sung-Hwan Kim*, Roh-Won Kim*, Hyeong-Soon Moon*,† and Myung-Hyun Kim**,†
*Precision Manufacturing & Control R&D Group, Korea Institute of Industrial Technology, Busan, 46742, Korea
**Dept. of Naval Architecture and Ocean Engineering, Pusan National University, Busan, 46241, Korea
Journal of Welding and Joining, Vol.37, No.4(2019) pp333-338
위에 논문은 주저자와 교신저자가 공동저자의 논문 시뮬레이션 및 논문 초안의 아이디어에 대한 기여를 적절히 고려하지 못한 잘못으로 인하여 본 논문의 공동저자로 누락하였기에 공동저자를 아래와 같이 추가하였습니다.
(저자 수정 후)
P-GMAW에서 용접 자세에 따른 비드 형상 및 재료 물성 변화에 관한 연구
박진형*·조대원**·김성환*·김노원*·문형순*,†·김명현***,†
*한국생산기술연구원 정밀가공제어그룹
**한국기계연구원 부산기계기술연구센터
***부산대학교 조선해양공학과
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW
Jin-Hyeong Park*, Dae Won Cho**, Sung-Hwan Kim*, Roh-Won Kim*, Hyeong-Soon Moon*,† and Myung-Hyun Kim***,†
*Precision Manufacturing & Control R&D Group, Korea Institute of Industrial Technology, Busan, 46742, Korea
**Busan Machinery Research Center, Korea Institute of Machinery and Materials, Busan, 46711, Korea
***Dept. of Naval Architecture and Ocean Engineering, Pusan National University, Busan, 46241, Korea
TOOLS
PDF Links  PDF Links
PubReader  PubReader
ePub Link  ePub Link
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
  Print
Share:      
METRICS
0
Crossref
820
View
72
Download
Related articles
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW  2019 August;37(4)
Study on the Fracture Toughness of FCA Weldment with the Yield Strength 420MPa Grade High Strength Steels for Offshore Structures Depending on the Welding Position  2018 April;36(2)
Influence of the Welding Speeds and Changing the Tool Pin Profiles on the Friction Stir Welded AA5083-O Joints   2017 June;35(3)
A Study on Surface and Cross-section Properties Depending on the Process Parameters of Laser Depositions with Metal Powders (SUS316L and IN718)  2017 June;35(3)
A Study on the Mechanical Properties of Heated Plates by Induction Heating System  2014 February;32(1)
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW  2019 August;37(4)
Study on the Fracture Toughness of FCA Weldment with the Yield Strength 420MPa Grade High Strength Steels for Offshore Structures Depending on the Welding Position  2018 April;36(2)
Influence of the Welding Speeds and Changing the Tool Pin Profiles on the Friction Stir Welded AA5083-O Joints   2017 June;35(3)
A Study on Surface and Cross-section Properties Depending on the Process Parameters of Laser Depositions with Metal Powders (SUS316L and IN718)  2017 June;35(3)
A Study on the Mechanical Properties of Heated Plates by Induction Heating System  2014 February;32(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.