Optimization of Weld-bonding Process Conditions of Dissimilar Materials Using Delta Spot Welding
Young-Hyun Kim*,**, Young-Gon Kim**, Dong-Cheol Kim***, Sung-Min Joo*
*Dept. Naval Architecture and Ocean Engineering, Graduate School, Chosun University, Gwangju, 61452, Korea
**Smart Manufacturing Process R&D Group, KITECH, Gwangju, 61012, Korea
***Joining R&D Group, KITECH, Incheon, 21999, Korea
Correspondence: Sung-Min Joo  Email: joo@chosun.ac.kr
Received March 15, 2019  Accepted April 11, 2019  Published online June 5, 2019
ABSTRACT
In the automobile industry, studies have been made on spot welds of non-ferrous metals such as aluminum, which has lightweight, high-strength, and excellent impact properties, in order to improve fuel efficiency through lightening of vehicle body weight. However, these dissimilar welds cause intermetallic compound formation and the galvanic corrosion in corrosion environments at the weld interface. On the other hand, it is known that the weld bonding process has the property of improving strength of spot welds by applying a structural adhesive between two metals and increasing the surface adhesive force. In this study, Al 6061-T6 with a thickness of 1mm and galvanized steel sheet (GA) with a grade of 440 MPa were used as target materials. As a process method, delta spot welding equipment was used for reducing the heat input using a special process tape and the weld bonding process by the D type structural adhesive was done. As a result, tensile shear strength after salt spray test for 1920 hours was more than twice that of spot welding condition and it was confirmed that the corrosion amount of the welds was lowered.
Keywords: GA440 | Al6061-T6 | Shearing stress | Weld nugget | Resistance spot welding | delta-spot welding | Weld-bonding process
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
34
View
0
Download
Related articles
Recent Study in Variation of Welding Materials for Overlay Welding  2013 December;31(6)
A Study on the Weldability and Mechanical Characteristics of Dissimilar Materials Butt Joints by Laser Assisted Friction Stir Welding  2010 December;28(6)
Optimization of Robot Welding Process of Subassembly Using Genetic Algorithm in the Shipbuilding  2009 April;27(2)
Effects of GMA Welding Conditions on the Bead Shape of Hardfacing Overlay Welding  2007 October;25(5)
Formation of Unmixed Zone in the Fusion Boundary of Dissimilar Metal Weld Zone  2007 August;25(4)
Recent Study in Variation of Welding Materials for Overlay Welding  2013 December;31(6)
A Study on the Weldability and Mechanical Characteristics of Dissimilar Materials Butt Joints by Laser Assisted Friction Stir Welding  2010 December;28(6)
Optimization of Robot Welding Process of Subassembly Using Genetic Algorithm in the Shipbuilding  2009 April;27(2)
Effects of GMA Welding Conditions on the Bead Shape of Hardfacing Overlay Welding  2007 October;25(5)
Formation of Unmixed Zone in the Fusion Boundary of Dissimilar Metal Weld Zone  2007 August;25(4)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.