The Effects of Nitrogen Content and Cold rolling reduction on the Mechanical Properties of New 420-series Stainless Steel Strip having a Mesh As-Welded Structure by the Electroslag Cladding
Jae-Young Jung*
*Automobile Parts & Materials Research Center, Kyungpook National University, Daegu, 41566, Korea
Correspondence: Jae-Young Jung  Email: jaeyjung7@gmail.com
Received August 10, 2017  Accepted September 26, 2017  Published online November 13, 2017
ABSTRACT
In this study, we investigated the mechanical properties of new 420 stainless steel strips as a function of nitrogen content and cold rolling reduction. Also, the results of the tensile and thermal fatigue tests using electroslag cladding specimens under a given welding condition were as follows. As-welded structures in which the delta ferrite is present in the form of a mesh are obtained in the alloy composition range in which about 5% delta ferrite is present in the Schaeffler diagram based on Cr equivalent and Ni equivalent. The softening temperature of new 420 stainless steel alloy designed as a mesh as-welded structure was determined to be 680-730℃ as a result of using cold rolled steel at 10-90% reduction. The ratio of 600℃ to room temperature tensile yield strength of weld metal was ~0.37 for the lowest N specimen and ~0.485 for the highest N specimen. However, high temperature ductility deteriorated with increasing N content. The presence of welding beads between the weld metal also reduced the elongation at room and high temperature rather than yield and tensile strength. The thermal fatigue characteristics are almost equal or better than those of the same materials prepared by the submerged welding method.
Keywords: Electroslag cladding | New 420-series stainless steel strip | A mesh as-welded structure | Martensite stainless steel overlay | Cold rolled strip
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1
Crossref
334
View
12
Download
Related articles
The Effects of Nitrogen Content and Cold Rolling Reduction on the Mechanical Properties of New 420-series Stainless Steel Strip having a Mesh As-Welded Structure by the Electroslag Cladding  2017 December;35(6)
Effects of Oxygen Contents in Shielding Gas on the Properties of Ferritic Stainless Steel GTA Weld  2010 October;28(5)
Effects of Nitrogen and Precipitates on the Mechanical Properties of 26Cr 2Mo Superferritic Stainless Steel Welds  2002 October;20(5)
The Effects of Nitrogen Content and Cold Rolling Reduction on the Mechanical Properties of New 420-series Stainless Steel Strip having a Mesh As-Welded Structure by the Electroslag Cladding  2017 December;35(6)
Effects of Oxygen Contents in Shielding Gas on the Properties of Ferritic Stainless Steel GTA Weld  2010 October;28(5)
Effects of Nitrogen and Precipitates on the Mechanical Properties of 26Cr 2Mo Superferritic Stainless Steel Welds  2002 October;20(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.