Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Principle of Resistance Welding and Analysis of Monitoring Results
조상명
JWJ. 1997;15(2):1-10.   Published online 1997 April 25

Excel Download

Monitoring resistance welding
Real-Time Weld Process Monitoring. 2008;238-259   Crossref logo
Link1 Link2 Link3

4788405 Weld thickness monitoring in resistance welding apparatus
Waste Management. 1991;11(3):I   Crossref logo
Link1 Link2

Monitoring of Dynamic Mechanical Parameters in Resistance Spot Welding of Aluminium
Welding in the World. 2005;49(1-2):17-21   Crossref logo
Link1 Link2 Link3

Monitoring of Resistance Spot Welding Process
Experimental Techniques. 2019;44(1):99-112   Crossref logo
Link1 Link2 Link3

Quality monitoring of resistance spot welding based on process parameters
Energy Procedia. 2012;14:925-930   Crossref logo
Link1 Link2

Development of Resistance Spot Welding Quality Monitoring Technology
Applied Mechanics and Materials. 2013;331:608-611   Crossref logo
Link1

An analysis of welding process monitoring and control
Real-Time Weld Process Monitoring. 2008;1-11   Crossref logo
Link1 Link2 Link3

Hopkinson rod test results and constitutive description of TRIP780 steel resistance spot welding material
Open Physics. 2020;18(1):961-967   Crossref logo
Link1 Link2

Feature Extraction and Analysis of Arc Sound Signal with Dynamic Welding Process
Key Technologies of Intelligentized Welding Manufacturing. 2020;17-35   Crossref logo
Link1

Resistance Spot Welding Characteristic of 1500MPa Steel Sheet Using Simulation (I) - Lobe Curve Characteristic Analysis of Resistance Spot Welding -