Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining. |
Determination of Optimal Weld Parameter for Joining Titanium Alloys by Gas Tungsten Arc Welding using Taguchi Method |
Nazmul Huda, Jae Won Kim, Changwook Ji, Dae-Geun Nam, Yeong-Do Park |
JWJ. 2021;39(1):81-88. Published online 2021 February 4 DOI: https://doi.org/10.5781/JWJ.2021.39.1.10 |
Determination of Optimal Weld Parameter for Joining Titanium Alloys by Gas Tungsten Arc Welding using Taguchi Method Gas-tungsten arc welding of magnesium alloys Activating flux tungsten inert gas welding of magnesium alloys Effect of Polarity and Oxide Fluxes on Weld-bead Geometry in Activated Tungsten Inert Gas (A-TIG) Welding A Study on the Estimation of Weld Quality Using the Thermal Images During Arc Welding Laser and Gas Metal Arc Based Dissimilar Joining of Automotive Aluminium Alloys and Steel Sheets - A Review Gas Metal Arc Lap Joining of Aluminium Alloys and Steel Sheets Weldability of wrought Haynes® 282® repair welded using manual gas tungsten arc welding Hybrid laser-arc welding of magnesium alloys Optimization of Weld Parameters and Weld Bead Dimensions in Welding of 0.3%C-Cr-Mo-V Steel by Gas Tungsten Arc Welding Process |
This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014. |