Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Pitting Corrosion Characteristic Depending on Welding Pass and Heat Input of GTA Weldment on Superaustenitic Stainless Steel(UNS S32654)
Dae-Hwan Ko, Young-Il. Park, Yong-Taek Shin
JWJ. 2020;38(6):528-534.   Published online 2020 December 24    DOI: https://doi.org/10.5781/JWJ.2020.38.6.2

Excel Download

Pitting Corrosion Characteristic Depending on Welding Pass and Heat Input of GTA Weldment on Superaustenitic Stainless Steel(UNS S32654)
Journal of Welding and Joining. 2020;38(6):528-534   Crossref logo
Link1 Link2 Link3

Heat Treatment Effect on Pitting Corrosion of Super Duplex Stainless Steel UNS S32750 GTA Welds
Advanced Materials Research. 2013;746:467-472   Crossref logo
Link1

Influence of heat input on the pitting corrosion and tensile behavior of GTA welded martensitic stainless steel (AISI410 SS) joints
Materials Today: Proceedings. 2021;   Crossref logo
Link1 Link2

Hot deformation characteristic and processing map of superaustenitic stainless steel S32654
Materials Science and Engineering: A. 2014;598:174-182   Crossref logo
Link1 Link2

Microsegregation-related pitting corrosion characteristics of AL-6XN superaustenitic stainless steel laser welds
Corrosion Science. 2010;52(10):3548-3553   Crossref logo
Link1 Link2

Pitting and crevice corrosion of superaustenitic stainless steels
Materials and Corrosion. 2004;55(3):164-173   Crossref logo
Link1 Link2 Link3

Localized corrosion of laser surface cladded UNS S31254 superaustenitic stainless steel on mild steel
Surface and Coatings Technology. 1997;88(1-3):90-95   Crossref logo
Link1 Link2

The effect of pulsed GTA welding on the residual stress of a stainless steel weldment
Journal of Materials Processing Technology. 2002;123(3):346-353   Crossref logo
Link1 Link2

Corrosion behaviour of a thin section martensitic stainless steel GTA weldment in chloride solutions
Materials Letters. 2008;62(17-18):2887-2890   Crossref logo
Link1 Link2

The Effect of Hydrogen on Pitting Corrosion of Superaustenitic and Austenitic-Ferritic Stainless Steels
Defect and Diffusion Forum. 2012;326-328:620-625   Crossref logo