Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Welding Process Improvement of 347H Stainless Steel Boiler Tube for Mitigating Reheat Cracking
Han-sang Lee, Hee-sun Kim, Myung-soo Park, Bum-shin Kim, Jong-min Lee
JWJ. 2020;38(6):551-562.   Published online 2020 December 1    DOI: https://doi.org/10.5781/JWJ.2020.38.6.5

Excel Download

Welding Process Improvement of 347H Stainless Steel Boiler Tube for Mitigating Reheat Cracking
Journal of Welding and Joining. 2020;38(6):551-562   Crossref logo
Link1 Link2 Link3

Automatic tube welding in boiler fabrication
Process Pipe and Tube Welding. 1991;76-88   Crossref logo
Link1 Link2 Link3

Study on Horizontal TIG Welding Process of 1Cr18Ni9Ti Stainless Steel Tube
Key Engineering Materials. 2018;777:377-380   Crossref logo
Link1

Welding residual stress analysis of 347H austenitic stainless steel boiler tubes using experimental and numerical approaches
Journal of Mechanical Science and Technology. 2016;30(4):1773-1779   Crossref logo
Link1 Link2 Link3

Ultra-high vacuum tight transition joints of titanium-stainless steel produced by explosive tube to tube welding. (Germany)
Vacuum. 1980;30(6):245   Crossref logo
Link1 Link2

Stress Corrosion Cracking Behaviour of Dissimilar Welding of AISI 310S Austenitic Stainless Steel to 2304 Duplex Stainless Steel
Metals. 2018;8(3):195   Crossref logo
Link1

Hot‐cracking susceptibility of fully austenitic stainless steel using pulsed‐current gas tungsten arc‐welding process
Engineering Reports. 2020;   Crossref logo
Link1 Link2 Link3

Influence of Second Thermal Cycle on Reheat Cracking Susceptibility of Welding CGHAZ in Vanadium-Modified 2.25Cr1Mo Steel
Procedia Engineering. 2015;130:487-496   Crossref logo
Link1 Link2

Thermo-Mechanical Simulation of Reheat Cracking in Welding CGHAZ of Vanadium-Modified 2.25Cr1Mo Steel
Applied Mechanics and Materials. 2015;750:178-185   Crossref logo
Link1

Reheat Cracking Susceptibility and Toughness of 2% CrMoWVNb P23 Steel Welds
Welding in the World. 2008;52(3-4):68-78   Crossref logo
Link1 Link2 Link3