Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of Ar Plasma Treatment for Surface of Insert Metal on Property of TLP Bonding Joint for Power Module
Seungju Baek, Dong-Yurl Yu, Jun-Hyuk Son, Junghwan Bang, Jungsoo Kim, Min-Su Kim, Han-Bo-Ram Lee, Yong-Ho Ko
JWJ. 2020;38(4):366-373.   Published online 2020 August 24    DOI: https://doi.org/10.5781/JWJ.2020.38.4.5

Excel Download

Effect of Ar Plasma Treatment for Surface of Insert Metal on Property of TLP Bonding Joint for Power Module
Journal of Welding and Joining. 2020;38(4):366-373   Crossref logo
Link1 Link2 Link3

The effect of grain boundary on the dissolution of base metal into insert metal during TLP bonding of Ni-base superalloys
Metals and Materials. 1999;5(5):477-484   Crossref logo
Link1 Link2 Link3

A Review on Recent Advances in Transient Liquid Phase (TLP) Bonding for Thermoelectric Power Module
REVIEWS ON ADVANCED MATERIALS SCIENCE. 2018;53(2):147-160   Crossref logo
Link1 Link2

Formation of Secondary Phases and Their Effect on the Mechanical Properties of Joints Formed by TLP Bonding Using Fe–B–Si Insert Metal in Duplex Stainless Steel
Metals and Materials International. 2018;25(2):425-438   Crossref logo
Link1 Link2 Link3

Effect of plasma treatment on interface property of BCN/GaN structure
Applied Surface Science. 2006;253(3):1459-1463   Crossref logo
Link1 Link2

Effect of plasma treatment on hydrophobicity and barrier property of polylactic acid
Surface and Coatings Technology. 2010;204(18-19):2933-2939   Crossref logo
Link1 Link2

Performance improvement in electrospun InGaZnO nanofibres field-effect-transistors using low thermal budget microwave calcination and Ar/O2 mixed-plasma surface treatment
Scientific Reports. 2020;10(1):   Crossref logo
Link1 Link2 Link3

Effects of austenite regeneration heat treatment on the TLP bonding of duplex stainless steel UNS S32750 using Fe-B-Si insert metal
Materials Chemistry and Physics. 2018;207:402-411   Crossref logo
Link1 Link2

Effect of bonding variables on TLP bonding of oxide dispersion strengthened superalloy
Journal of Materials Science. 2007;42(22):9187-9193   Crossref logo
Link1 Link2 Link3 Link4

Surface treatment methods
Surface Treatment in Bonding Technology. 2019;47-62   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.