Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
A Study on the Effect of Plating Layer on the Corrosion Properties of Steel/Al Dissimilar Magnetic Pulse Weldments
Byoung-Hyun Yoon, Ji-Yeon Shim, Bong-Yong Kang
JWJ. 2020;38(3):305-310.   Published online 2020 June 1    DOI: https://doi.org/10.5781/JWJ.2020.38.3.11

Excel Download

A Study on the Effect of Plating Layer on the Corrosion Properties of Steel/Al Dissimilar Magnetic Pulse Weldments
Journal of Welding and Joining. 2020;38(3):305-310   Crossref logo
Link1 Link2 Link3

Effect of Pulse Duration on Corrosion and Impression Creep Properties of AA5083-H111 Al-Mg Alloy Weldments Processed by P-GTAW
Advanced Engineering Materials. 2018;20(6):1701147   Crossref logo
Link1 Link2

Stress Corrosion Cracking of Austenitic Stainless Steel Weldments
Corrosion of Austenitic Stainless Steels. 2002;166-189   Crossref logo
Link1 Link2 Link3

Intergranular corrosion susceptibility in supermartensitic stainless steel weldments
Corrosion Science. 2009;51(10):2316-2323   Crossref logo
Link1 Link2

Microstructures and mechanical properties of dissimilar T91/347H steel weldments
Journal of Materials Processing Technology. 2015;220:76-86   Crossref logo
Link1 Link2

Study on corrosion resistance of palladium films on 316L stainless steel by electroplating and electroless plating
Corrosion Science. 2008;50(10):2873-2878   Crossref logo
Link1 Link2

Mechanical and corrosion behaviours of dissimilar weldments of modified 9Cr-1Mo steel to 316LN stainless steel through spark plasma sintering
Materials Today: Proceedings. 2020;27:2657-2660   Crossref logo
Link1 Link2

Microstructure, mechanical properties and corrosion behavior of laser welded dissimilar joints between ferritic stainless steel and carbon steel
Materials & Design (1980-2015). 2015;65:855-861   Crossref logo
Link1 Link2

Magnetic properties of alloy films prepared by fast pulse-plating
Journal of Magnetism and Magnetic Materials. 2001;226-230:1650-1652   Crossref logo
Link1 Link2

Comparative studies on the corrosion properties of a Fe–Mn–Al–Si steel and an interstitial-free steel
Corrosion Science. 2008;50(10):2879-2884   Crossref logo
Link1 Link2