Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of Laser Power Feedback Control on Mechanical Properties of Stainless Steel Part Built by Direct Energy Deposition
ChiYen Kim, JiSung Kim, Ho Lee, MinKyu Park, SungWook Kim, SeongSeon Shin, JunHo Hwang, HyunDeok Kim
JWJ. 2020;38(2):197-202.   Published online 2020 April 3    DOI: https://doi.org/10.5781/JWJ.2020.38.2.10

Excel Download

Influences of deposition strategies and oblique angle on properties of AISI316L stainless steel oblique thin-walled part by direct laser fabrication
Optics & Laser Technology. 2016;80:138-144   Crossref logo
Link1 Link2

Direct laser deposition with different types of 316L steel particle: A comparative study of final part properties
Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture. 2013;227(4):520-531   Crossref logo
Link1 Link2 Link3

Laser Metal Deposition Influence on the Mechanical Properties of Steels and Stainless Steel Composites: A Review
Materials Today: Proceedings. 2018;5(9):18603-18620   Crossref logo
Link1 Link2

Cracking behavior and mechanical properties of austenitic stainless steel parts produced by laser metal deposition
Materials & Design. 2013;45:228-235   Crossref logo
Link1 Link2

Effect of build geometry and orientation on microstructure and properties of additively manufactured 316L stainless steel by laser metal deposition
Materialia. 2019;7:100359   Crossref logo
Link1 Link2

Laser-assisted direct joining of AISI304 stainless steel with polycarbonate sheets: Thermal analysis, mechanical characterization, and bonds morphology
Optics & Laser Technology. 2017;88:205-214   Crossref logo
Link1 Link2

The structure and mechanical properties of parts elaborated by direct laser deposition 316L stainless steel powder obtained in various ways
Journal of Physics: Conference Series. 2017;941:012040   Crossref logo
Link1 Link2 Link3 Link4

Microstructure and mechanical properties of stainless steel 316L obtained by Direct Metal Laser Deposition
Journal of Physics: Conference Series. 2019;1238:012029   Crossref logo
Link1 Link2 Link3 Link4

Functionally Graded Stainless Steel Fabricated by Direct Laser Deposition: Anisotropy of Mechanical Properties and Hardness
Acta Metallurgica Sinica (English Letters). 2017;31(1):19-26   Crossref logo
Link1 Link2 Link3

Effect of laser remelting processing on microstructure and mechanical properties of 17-4 PH stainless steel during laser direct metal deposition
Journal of Materials Processing Technology. 2020;284:116738   Crossref logo
Link1 Link2