CrossRef Text and Data Mining
Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
The Effect of Pre-Welding on Nugget Growth Behavior and Weldability for the Resistance Spot Welding of A6014 - T4 Alloy
Hyun-Uk Jun, Jae-Hun Kim, Joo-Yong Cheon, Young-Gon Kim, Yang-Do Kim, Changwook Ji
JWJ. 2020;38(2):203-210.   Published online 2020 March 11    DOI: https://doi.org/10.5781/JWJ.2020.38.2.11

Excel Download

Influence of Welding Conditions on Nugget Formation in Single-Sided Resistance Spot Welding Process
Welding in the World. 2009;53(5-6):15-22   Crossref logo
Link1 Link2 Link3

Study on the Mechanism of Nugget Growth Behavior in Three Sheets Stack Resistance Spot Welding
Journal of Welding and Joining. 2019;37(6):564-571   Crossref logo
Link1 Link2 Link3

Resistance Spot Welding Characteristic of 1500MPa Steel Sheet Using Simulation (II) - Estimation Model for Nugget Diameter of Resistance Spot Welds -
Journal of Welding and Joining. 2018;36(3):51-56   Crossref logo
Link1 Link2 Link3

Hybrid Nugget Diameter Prediction for Resistance Spot Welding
Procedia Manufacturing. 2018;17:395-402   Crossref logo
Link1 Link2

Resistance spot weldability and high cycle fatigue behaviour of martensitic (M190) steel sheet
Fatigue & Fracture of Engineering Materials & Structures. 2010;34(1):46-52   Crossref logo
Link1

Numerical and experimental study of nugget size growth in resistance spot welding of austenitic stainless steels
Journal of Materials Processing Technology. 2012;212(2):347-354   Crossref logo
Link1 Link2

Optimization of Electrical Resistance Spot Welding and Comparison with Friction Stir Spot Welding of AA2024-T3 Aluminum Alloy Joints
Materials Today: Proceedings. 2017;4(2):1762-1771   Crossref logo
Link1 Link2

Resistance spot welding of galvanized steel: Part II. Mechanisms of spot weld nugget formation
Metallurgical Transactions B. 1986;17(4):887-901   Crossref logo
Link1 Link2 Link3

Comparing the weldability of AA6013-T4 aluminium alloy on DP600 dual-phase steel with laser welding and resistance spot welding
Journal of the Brazilian Society of Mechanical Sciences and Engineering. 2020;42(1):   Crossref logo
Link1 Link2 Link3

Effects of Electrode Face Radius and Force on Resistance Spot Weldability of Aluminium Alloy 6061
Journal of Welding and Joining. 2018;36(6):46-51   Crossref logo
Link1 Link2 Link3

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.