Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Study on the Initial Design of an LNG Fuel Tank using 9 wt.% Nickel Steel for Ships and Performance Evaluation of the Welded Joint
Bo Eun Kim, Jeong-Yeol Park, Jeong Soo Lee, Myung-Hyun Kim
JWJ. 2019;37(6):555-563.   Published online 2019 December 30    DOI: https://doi.org/10.5781/JWJ.2019.37.6.4

Excel Download

Study on the Initial Design of an LNG Fuel Tank using 9 wt.% Nickel Steel for Ships and Performance Evaluation of the Welded Joint
Journal of Welding and Joining. 2019;37(6):555-563   Crossref logo
Link1 Link2 Link3

Effect of joint design on ballistic performance of quenched and tempered steel welded joints
Materials & Design (1980-2015). 2014;54:616-623   Crossref logo
Link1 Link2

Experimental investigations of fracture and fatigue crack growth of copper–steel joints arc welded using nickel-base filler
Materials & Design. 2015;67:244-260   Crossref logo
Link1 Link2

Metallurgical and mechanical examinations of steel–copper joints arc welded using bronze and nickel-base superalloy filler materials
Materials & Design. 2013;47:793-809   Crossref logo
Link1 Link2

Welded joint design
Journal of Constructional Steel Research. 1988;9(3):229   Crossref logo
Link1 Link2

Basis of design of welded structures
Welded Joint Design. 1999;45-51   Crossref logo
Link1 Link2 Link3

Development of 9% Nickel Steel for LNG Applications
steel research international. 2007;78(3):189-194   Crossref logo
Link1 Link2 Link3

Study on buckling of convex fillet welded joint
Steel Research. 1996;67(6):235-239   Crossref logo
Link1 Link2 Link3

Case Study 2: Hatch Corner Design for Container Ships
Fatigue Analysis of Welded Components. 2006;36-39   Crossref logo
Link1 Link2 Link3

Tank Analysis
Design and Construction of LNG Storage Tanks. 2019;59-75   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.