Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Validation of the Master Curve Approach Based on Charpy Impact Test with Groove Shapes
Jin-Ho Lee, Young-Taek Shin, Myung-Hyun Kim
JWJ. 2019;37(6):539-546.   Published online 2019 December 18    DOI: https://doi.org/10.5781/JWJ.2019.37.6.2

Excel Download

Validation of the Master Curve Approach Based on Charpy Impact Test with Groove Shapes
Journal of Welding and Joining. 2019;37(6):539-546   Crossref logo
Link1 Link2 Link3

Modeling Charpy impact energy of functionally graded steel based on the strain gradient plasticity theory and modified stress–strain curve data
Computational Materials Science. 2011;50(12):3350-3357   Crossref logo
Link1 Link2

Simulation Charpy impact energy of functionally graded steels by modified stress–strain curve through mechanism-based strain gradient plasticity theory
Computational Materials Science. 2012;51(1):225-232   Crossref logo
Link1 Link2

Charpy trend-curve development based on PWR surveillance data
Nuclear Engineering and Design. 1985;86(1):79-86   Crossref logo
Link1 Link2

Evaluation of dynamic fracture toughness parameters of locomotive axle steel by instrumented Charpy impact test
Fatigue & Fracture of Engineering Materials & Structures. 2016;40(4):512-522   Crossref logo
Link1 Link2 Link3

Direct measurement of reactor pressure vessel steels fracture toughness: Master Curve concept and instrumented Charpy-V test
International Journal of Pressure Vessels and Piping. 2000;77(10):605-612   Crossref logo
Link1 Link2

Estimation of fracture toughness of 16MnDR steel using Master Curve method and Charpy V-notch impact energy
Theoretical and Applied Fracture Mechanics. 2018;96:443-451   Crossref logo
Link1 Link2

Analysis of impact properties of 3D-carbon-carbon composite materials by the instrumented Charpy test
Composites. 1987;18(2):180   Crossref logo
Link1 Link2

Specimen loading determined by displacement measurement in instrumented Charpy impact test
Engineering Fracture Mechanics. 2000;65(6):703-713   Crossref logo
Link1 Link2

Confidence Interval Assessment for Charpy Impact Energy Predictions – A Gaussian Mixture Model (GMM)-Based Approach