CrossRef Text and Data Mining
Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of the Laser Beam Spot Size and Process Parameters on the Cross Section of SUS316L Parts using DED(Directed Energy Deposition)
SeongSeon Shin, JongHoon Lee, SungWook Kim, JunHo Hwang, HyunDeok Kim
JWJ. 2019;37(5):508-513.   Published online 2019 October 25    DOI: https://doi.org/10.5781/JWJ.2019.37.5.11

Excel Download

Effect of the Laser Beam Spot Size and Process Parameters on the Cross Section of SUS316L Parts using DED(Directed Energy Deposition)
Journal of Welding and Joining. 2019;37(5):508-513   Crossref logo
Link1 Link2 Link3

In-process measurement of melt pool cross-sectional geometry and grain orientation in a laser directed energy deposition additive manufacturing process
Optics & Laser Technology. 2020;129:106280   Crossref logo
Link1 Link2

Optimisation of process parameters for deposition of colmonoy using directed energy deposition process
Materials Today: Proceedings. 2020;26:1108-1112   Crossref logo
Link1 Link2

An experimental study on microstructural characteristics and mechanical properties of stainless-steel 316L parts using directed energy deposition (DED) process
Journal of Mechanical Science and Technology. 2019;33(12):5731-5737   Crossref logo
Link1 Link2 Link3

Modeling analysis of grain morphologies in Directed energy deposition (DED) coating with different laser scanning patterns
Materials Letters. 2019;251:8-12   Crossref logo
Link1 Link2

Development and evaluation of a dynamic powder splitting system for the directed energy deposition (DED) process
CIRP Annals. 2020;   Crossref logo
Link1 Link2

Effect of layer thickness setting on deposition characteristics in direct energy deposition (DED) process
Optics & Laser Technology. 2016;86:69-78   Crossref logo
Link1 Link2

Effect of laser spot size on energy balance in laser induced plasmas. (USA)
Vacuum. 1981;31(6):272   Crossref logo
Link1 Link2

Laser Beam Energy as Weapon
Directed-Energy Beam Weapons. 2019;239-268   Crossref logo
Link1

Laser direct metal deposition process of thin-walled parts using variable spot by inside-beam powder feeding
Rapid Prototyping Journal. 2018;24(1):18-27   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.