Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Experimental Investigation of Infrared Laser Drilling Process Applied with Different Repetition Rate on Ni-Au Coated BeCu
Seungik Son, Dongkyoung Lee
JWJ. 2019;37(3):206-211.   Published online 2019 June 27    DOI: https://doi.org/10.5781/JWJ.2019.37.3.2

Excel Download

Experimental Investigation of Infrared Laser Drilling Process Applied with Different Repetition Rate on Ni-Au Coated BeCu
Journal of Welding and Joining. 2019;37(3):206-211   Crossref logo
Link1 Link2 Link3

Experimental Investigation of Process Parameters in Drilling LM25 Composites Coated with Multi Wall Carbon Nano Tubes Using Sonication Process
Archives of Metallurgy and Materials. 2017;62(3):1761-1770   Crossref logo
Link1 Link2

Model of the absorption variation during pulsed laser heating applied to welding of electronic Au/Ni-coated Cu-leadframes
Applied Surface Science. 2005;241(3-4):362-370   Crossref logo
Link1 Link2

Experimental Investigation of Laser Spot Welding of Ni and Au-Sn-Ni Alloy
Journal of Welding and Joining. 2017;35(2):1-5   Crossref logo
Link1 Link2 Link3

Experimental optimization of the repetition rate difference in dual-comb ranging system
Applied Physics Express. 2014;7(10):106602   Crossref logo
Link1 Link2 Link3 Link4 Link5

Charge-Line Dual-FET High-Repetition-Rate Pulsed Laser Driver
Applied Sciences. 2019;9(7):1289   Crossref logo
Link1

High repetition rate CH4 laser
International Journal of Infrared and Millimeter Waves. 1982;3(2):153-157   Crossref logo
Link1 Link2 Link3

Comparison on different repetition rate locking methods in Er-doped fiber laser
Laser Physics. 2018;28(5):055108   Crossref logo
Link1 Link2 Link3 Link4

Experimental and Numerical Investigation of Temperature Distribution and Hole Geometry during Laser Drilling Process
Procedia Engineering. 2015;100:384-393   Crossref logo
Link1 Link2

High Repetition-Rate Laser Z-Scan Measurements: Criterion for Recognizing Adverse Thermal Effects
Applied Physics Research. 2019;11(2):73   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.