Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Experimental Investigation of Laser Cutting on Cement Composites
Youngjin Seo, Sukhoon Pyo, Dongkyoung Lee
JWJ. 2019;37(3):226-230.   Published online 2019 June 27    DOI: https://doi.org/10.5781/JWJ.2019.37.3.5

Excel Download

Experimental investigation into early age shrinkage of cement paste by using fibre Bragg gratings
Cement and Concrete Composites. 2004;26(5):473-479   Crossref logo
Link1 Link2

Experimental Investigation of Multi-mode Fiber Laser Cutting of Cement Mortar
Materials. 2018;11(2):278   Crossref logo
Link1

Mechanical behaviour of ferrocement composites: an experimental investigation
Cement and Concrete Composites. 1999;21(4):301-312   Crossref logo
Link1 Link2

Laser cutting of polymeric materials: An experimental investigation
Optics & Laser Technology. 2010;42(3):503-508   Crossref logo
Link1 Link2

Experimental Investigation of Laser Cutting on Cement Composites
Journal of Welding and Joining. 2019;37(3):226-230   Crossref logo
Link1 Link2 Link3

Experimental investigation of compressive strength and compressive fracture energy of longitudinally cracked concrete
Cement and Concrete Composites. 2018;93:1-18   Crossref logo
Link1 Link2

Experimental and analytical investigation of ferrocement–concrete composite beams
Cement and Concrete Composites. 2004;26(7):787-796   Crossref logo
Link1 Link2

Experimental investigation into the compressive strength development of cemented paste backfill containing Nano-silica
Cement and Concrete Composites. 2016;72:180-189   Crossref logo
Link1 Link2

Experimental investigation of the effect of process parameters on cutting region temperature and cutting edge quality in laser cutting of AL6061T6 alloy
Optik. 2019;184:457-463   Crossref logo
Link1 Link2

Investigation of the electromagnetic characteristics of cement based composites filled with EPS
Cement and Concrete Composites. 2007;29(1):49-54   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.