Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
The Effects of Heat Treatment Temperature on Wear Characteristics of Hyper-Eutectic Al-Si Alloy Laser Clad Layer
Hyoung-Keun Lee
JWJ. 2019;37(3):262-267.   Published online 2019 June 10    DOI: https://doi.org/10.5781/JWJ.2019.37.3.10

Excel Download

The Effects of Heat Treatment Temperature on Wear Characteristics of Hyper-Eutectic Al-Si Alloy Laser Clad Layer
Journal of Welding and Joining. 2019;37(3):262-267   Crossref logo
Link1 Link2 Link3

The influence of start–stop transient velocity on the friction and wear behaviour of a hyper-eutectic Al–Si automotive alloy
Wear. 2013;306(1-2):209-218   Crossref logo
Link1 Link2

Effect of humidity on friction and wear of AlSi eutectic alloy and AlSi alloy-graphite composites
Wear. 1996;198(1-2):169-175   Crossref logo
Link1 Link2

Microstructural Evolution of Cast Hyper-Eutectic Al-18% Si Alloy during Cyclic Semi-Solid Heat Treatment
Journal of Minerals and Materials Characterization and Engineering. 2015;03(05):390-398   Crossref logo
Link1 Link2

Effect of Roughness of Hypo-and Hyper-Eutectic Al-Si Piston Alloy on Wear Characteristics under Lubrication
Procedia Engineering. 2013;53:616-623   Crossref logo
Link1 Link2

Microstructure and sliding wear resistance of an Al–12wt.% Si/TiC laser clad coating
Wear. 2012;282-283:31-39   Crossref logo
Link1 Link2

Improvement in wear resistance of hyper-eutectic AlSi cast alloy by laser surface remelting
Surface and Coatings Technology. 2003;169-170:468-471   Crossref logo
Link1 Link2

Wear behaviours of laser-clad stellite alloy 6
Wear. 1996;192(1-2):78-84   Crossref logo
Link1 Link2

Effects of T6 heat treatment on mechanical, abrasive and erosive-corrosive wear properties of eutectic Al–Si alloy
Transactions of Nonferrous Metals Society of China. 2012;22(5):1041-1050   Crossref logo
Link1 Link2

Effects of sliding speed on the unlubricated wear behaviour of Al-12.3wt.%Si alloy
Wear. 1991;151(1):97-110   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.