Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Optimization of Painting Process to Improve Durability of Mega Yacht and Cavitation Erosion Characteristics
Il-Cho Park, Min-Su Han, Seong-Jong Kim
JWJ. 2019;37(3):254-261.   Published online 2019 June 10    DOI: https://doi.org/10.5781/JWJ.2019.37.3.9

Excel Download

Optimization of Painting Process to Improve Durability of Mega Yacht and Cavitation Erosion Characteristics
Journal of Welding and Joining. 2019;37(3):254-261   Crossref logo
Link1 Link2 Link3

Influence of galvanic macro-cell corrosion on the cavitation erosion durability assessment of metallic materials—International cavitation erosion test of Gdańsk
Wear. 1995;186-187:542-547   Crossref logo
Link1 Link2

Cavitation erosion behavior in seawater of electroless Ni-P coating and process optimization using Taguchi method
Applied Surface Science. 2019;477:37-43   Crossref logo
Link1 Link2

Painting process boosts production output, imparts surface durability to frp components
Composites. 1974;5(6):272   Crossref logo
Link1 Link2

The bubble bursts for cavitation in natural rivers: laboratory experiments reveal minor role in bedrock erosion
Earth Surface Processes and Landforms. 2017;42(9):1308-1316   Crossref logo
Link1 Link2

Phenomenological prediction tool for cavitation erosion fed with the International Cavitation Erosion Test results
Wear. 2016;364-365:1-9   Crossref logo
Link1 Link2

Corrosion fatigue of steel under cavitation erosion generated intermittently in 3% salt water (results of two-stage tests with and without cavitation erosion)
Wear. 1984;96(1):85-98   Crossref logo
Link1 Link2

Cavitation erosion of aluminum considering bubble collapse, pulse height spectra and cavitation erosion efficiency
Wear. 1979;55(2):221-234   Crossref logo
Link1 Link2

Relationship between the geometric features of carbon steel cavitation erosion debris and the cavitation erosion stages
Chinese Science Bulletin. 2010;55(7):670-676   Crossref logo
Link1 Link2 Link3

Cavitation erosion testing of polymers
Wear. 1967;10(3):259   Crossref logo
Link1 Link2