CrossRef Text and Data Mining
Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Optimization of Weld-bonding Process Conditions of Dissimilar Materials using Delta Spot Welding
Young-Hyun Kim, Young-Gon Kim, Dong-Cheol Kim, Sung-Min Joo
JWJ. 2019;37(3):231-236.   Published online 2019 June 5    DOI: https://doi.org/10.5781/JWJ.2019.37.3.6

Excel Download

Optimization of Weld-bonding Process Conditions of Dissimilar Materials using Delta Spot Welding
Journal of Welding and Joining. 2019;37(3):231-236   Crossref logo
Link1 Link2 Link3

Optimization of CO2 Laser Beam Welding Process Parameters to Attain Maximum Weld Strength in Dissimilar Metals
Materials Today: Proceedings. 2018;5(2):6607-6616   Crossref logo
Link1 Link2

Optimization of resistance spot welding process parameters in dissimilar joint of MS and ASS 304 sheets
Materials Today: Proceedings. 2020;26:1284-1288   Crossref logo
Link1 Link2

Influence of Welding Conditions on Nugget Formation in Single-Sided Resistance Spot Welding Process
Welding in the World. 2009;53(5-6):15-22   Crossref logo
Link1 Link2 Link3

Optimization of welding parameters for friction stir spot welding of AA6062 with similar and dissimilar thicknesses
Materials Today: Proceedings. 2019;19:251-255   Crossref logo
Link1 Link2

Exploring the electrodes alignment and mushrooming effects on weld geometry of dissimilar steels during the spot welding process
Sadhana. 2014;39(6):1563-1572   Crossref logo
Link1 Link2 Link3

Parametric optimization of resistance spot welding for multi spot welded lap shear specimen to predict weld strength
Materials Today: Proceedings. 2019;19:700-707   Crossref logo
Link1 Link2

Some studies on weld bead geometries for laser spot welding process using finite element analysis
Materials & Design. 2012;34:412-426   Crossref logo
Link1 Link2

Optimization of process parameters in welding of dissimilar steels using robot TIG welding
IOP Conference Series: Materials Science and Engineering. 2018;330:012096   Crossref logo
Link1 Link2 Link3 Link4

Optimization of welding current waveform for dissimilar material with DP590 and Al5052 by Delta-spot welding process
Journal of Mechanical Science and Technology. 2016;30(6):2713-2721   Crossref logo
Link1 Link2 Link3

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.