Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of Air-HAST Conditions on Sn Whisker Growth
Chulmin Oh, Sangjoo Oh, Dajung Kim, Won Sik Hong, Keun-Soo kIM
JWJ. 2019;37(2):21-25.   Published online 2019 April 22    DOI: https://doi.org/10.5781/JWJ.2019.37.2.4

Excel Download

Effect of Air-HAST Conditions on Sn Whisker Growth
Journal of Welding and Joining. 2019;37(2):21-25   Crossref logo
Link1 Link2 Link3

Effect of Environmental Conditions on Tin (Sn) Whisker Growth
Engineering. 2015;07(12):816-826   Crossref logo
Link1 Link2 Link3

The Effect of Micro-Alloying of Sn Plating on Mitigation of Sn Whisker Growth
Journal of Electronic Materials. 2009;38(12):2726-2734   Crossref logo
Link1 Link2 Link3

Investigation of Sn Whisker Growth in Electroplated Sn and Sn-Ag as a Function of Plating Variables and Storage Conditions
Journal of Electronic Materials. 2013;43(1):259-269   Crossref logo
Link1 Link2 Link3

Effect of adding Ge on rapid whisker growth of Sn–3Ag–0.5Cu–0.5Ce alloy
Journal of Alloys and Compounds. 2009;480(2):974-980   Crossref logo
Link1 Link2

Rapid whisker growth on the surface of Sn–3Ag–0.5Cu–1.0Ce solder joints
Scripta Materialia. 2006;55(11):983-986   Crossref logo
Link1 Link2

Topics in Lead-Free Solders: Interfacial and Sn Whisker Growth
JOM. 2012;64(10):1174-1175   Crossref logo
Link1 Link2 Link3

Mitigation of Sn Whisker Growth by Composite Ni/Sn Plating
Journal of Electronic Materials. 2009;38(12):2516-2524   Crossref logo
Link1 Link2 Link3

Tin (Sn) whisker growth from electroplated Sn finished
IOP Conference Series: Materials Science and Engineering. 2019;701:012005   Crossref logo
Link1 Link2 Link3 Link4

Effect of Cu Substrate Roughness and Sn Layer Thickness on Whisker Development from Sn Thin-Films
Materials. 2019;12(21):3609   Crossref logo
Link1

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.