Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Microtexture and Microstructural Evolution of Friction Stir Welded AA5052-H32 Joints
Young-Bin Lim, Kwang-Jin Lee
JWJ. 2019;37(2):35-40.   Published online 2019 March 26    DOI: https://doi.org/10.5781/JWJ.2019.37.2.6

Excel Download

Microtexture and Microstructural Evolution of Friction Stir Welded AA5052-H32 Joints
Journal of Welding and Joining. 2019;37(2):35-40   Crossref logo
Link1 Link2 Link3

Tool Pin Profile Studies on Friction Stir Welded Joints of AA5052-H32 and AA6061-T6 Aluminum Alloys
Advances in Manufacturing Processes. 2018;663-670   Crossref logo
Link1

Microstructural and Mechanical Investigations of Friction Stir Welded TI/TI- And TI-Alloy/TI-Alloy-Joints
Friction Stir Welding and Processing VII. 2013;141-149   Crossref logo
Link1

Establishing Mathematical Relationships to Study Tensile Behavior of Friction Stir Welded AA5086-H32 Aluminium Alloy Joints
Silicon. 2018;11(1):51-65   Crossref logo
Link1 Link2 Link3

Effect of rotational speed on friction stir spot welding of AA5052-H32/HDPE/AA5052-H32 sandwich sheets
Journal of Materials Processing Technology. 2018;252:511-523   Crossref logo
Link1 Link2

Influence of Tool Plunge Depth During Friction Stir Spot Welding of AA5052-H32/HDPE/AA5052-H32 Sandwich Sheets
Strengthening and Joining by Plastic Deformation. 2018;95-121   Crossref logo
Link1

Friction stir spot welding of AA5052-H32/HDPE/AA5052-H32 sandwich sheets at varying plunge speeds
Thin-Walled Structures. 2019;138:415-429   Crossref logo
Link1 Link2

Tensile properties of friction stir welded and friction stir welded-superplastically formed Ti–6Al–4V butt joints
Materials & Design. 2010;31(6):3056-3061   Crossref logo
Link1 Link2

Evolution of Microstructure and Microtexture in Friction Stir Welded Oxide Dispersion Strengthened Steel
Microscopy and Microanalysis. 2013;19(S2):714-715   Crossref logo
Link1

Effect of Tool Rotation Speed on Friction Stir Spot Welded AA5052-H32 and AA6082-T6 Dissimilar Aluminum Alloys
Metallography, Microstructure, and Analysis. 2016;5(2):142-148   Crossref logo
Link1 Link2 Link3