Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Nucleation Behavior of Acicular Ferrite in 1 GPa Class High Strength Steel Weld Metal
Yongjoon Kang, Changhee Lee
JWJ. 2019;37(1):21-26.   Published online 2019 February 19    DOI: https://doi.org/10.5781/JWJ.2019.37.1.3

Excel Download

Nucleation Behavior of Acicular Ferrite in 1 GPa Class High Strength Steel Weld Metal
Journal of Welding and Joining. 2019;37(1):21-26   Crossref logo
Link1 Link2 Link3

Inclusion Characteristics and Acicular Ferrite Nucleation in Ti-Containing Weld Metals of X70 Pipeline Steel
steel research international. 2017;89(2):1700316   Crossref logo
Link1 Link2

Influence of Ti on non-metallic inclusion formation and acicular ferrite nucleation in high-strength low-alloy steel weld metals
Metals and Materials International. 2014;20(1):119-127   Crossref logo
Link1 Link2 Link3

Low-temperature mechanical behavior of an “acicular” ferrite HSLA (high strength-low alloy) line pipe steel
Metallurgical Transactions A. 1979;10(12):1941-1944   Crossref logo
Link1 Link2 Link3

Grain Size of Acicular Ferrite in Ferritic Weld Metal
Welding in the World. 2011;55(9-10):36-40   Crossref logo
Link1 Link2 Link3 Link4

Fracture Assessment of the Weld–Base Metal Interface of High-Strength Steel Weld Joint
Strength of Materials. 2018;50(1):11-19   Crossref logo
Link1 Link2 Link3

Effect of Ti-containing inclusions on the nucleation of acicular ferrite and mechanical properties of multipass weld metals
Micron. 2013;45:107-114   Crossref logo
Link1 Link2

Effect of weld metal composition and welding conditions on δ -ferrite and CVN toughness of austenitic-ferritic weld metal
Steel Research. 1985;56(3):163-166   Crossref logo
Link1 Link2 Link3

High-strength, ductile Mn-Mo-Nb steels with a structure of acicular ferrite
Metal Science and Heat Treatment. 1976;18(1):59-65   Crossref logo
Link1 Link2 Link3

Factors Affecting the Inclusion Potency for Acicular Ferrite Nucleation in High-Strength Steel Welds
Metallurgical and Materials Transactions A. 2016;47(6):2842-2854   Crossref logo
Link1 Link2 Link3