Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of Burn-off Length on the Properties of Friction Welded Dissimilar Steel Bars
Muralimohan Cheepu, Woo Seong Che
JWJ. 2019;37(1):46-55.   Published online 2019 January 18    DOI: https://doi.org/10.5781/JWJ.2019.37.1.6

Excel Download

Effect of Burn-off Length on the Properties of Friction Welded Dissimilar Steel Bars
Journal of Welding and Joining. 2019;37(1):46-55   Crossref logo
Link1 Link2 Link3

Microstructural characterization and mechanical properties of friction-stir-welded dissimilar lap joint of CP-Ti and steel
Proceedings of the 1st International Joint Symposium on Joining and Welding. 2013;259-265   Crossref logo
Link1 Link2

An Analysis of Microstructure and Mechanical Properties on Friction Stir Welded Joint of Dissimilar 304 Stainless Steel and Commercially Pure Aluminium
Archives of Metallurgy and Materials. 2017;62(3):1813-1817   Crossref logo
Link1 Link2

Corrosion Properties of Dissimilar Friction Stir Welded 6061 Aluminum and HT590 Steel
Metals and Materials International. 2018;24(6):1232-1240   Crossref logo
Link1 Link2 Link3

Study of the Weld Zone of Friction Welded C45/1.3344PM Dissimilar Steel Joints
Design, Fabrication and Economy of Welded Structures. 2008;469-475   Crossref logo
Link1 Link2 Link3

Fatigue behaviour of friction welded medium carbon steel and austenitic stainless steel dissimilar joints
Materials & Design. 2011;32(4):1888-1894   Crossref logo
Link1 Link2

An Investigation on the Effect of Axial Pressures on the Mechanical Properties of Friction Welded Dissimilar Steels
Advances in Mechanical Engineering. 2014;6:639378   Crossref logo
Link1 Link2 Link3

Effect of Tool Rotational Speeds on the Microstructure and Mechanical Properties of a Dissimilar Friction-Stir-Welded CuCrZr/CuNiCrSi Butt Joint
Metals. 2018;8(7):526   Crossref logo
Link1

Effect of pin length on Friction Stir Spot Welding (FSSW) of dissimilar Aluminum-steel joints
Procedia Materials Science. 2015;9:504-513   Crossref logo
Link1 Link2

Effect of Welding Parameters on the Microstructure and Mechanical Properties of a Friction Stir Welded 11CR-Ferritic/Martensitic Steel
Friction Stir Welding and Processing VII. 2013;91-99   Crossref logo
Link1

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.