Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Brittle Crack Propagation Path Due to the Effect of Welding Residual Stresses
Gyubaek An, Hongyeol Bae, Jeongung Park, Wan Chuck Woo
JWJ. 2018;36(6):21-27.   Published online 2018 December 13    DOI: https://doi.org/10.5781/JWJ.2018.36.6.4

Excel Download

Brittle Crack Propagation Path Due to the Effect of Welding Residual Stresses
Journal of Welding and Joining. 2018;36(6):21-27   Crossref logo
Link1 Link2 Link3

RESIDUAL STRESSES AND FRETTING, CRACK INITIATION AND PROPAGATION
Residual Stresses. 1987;511-525   Crossref logo
Link1 Link2

Effect of welding residual stresses on fatigue crack growth thresholds
International Journal of Fatigue. 2013;50:10-17   Crossref logo
Link1 Link2

Interaction of welding residual stresses and warm pre-stressing on brittle fracture of a pipe containing an internal semi-elliptical crack
Engineering Failure Analysis. 2015;52:116-128   Crossref logo
Link1 Link2

RESIDUAL STRESSES AS A CONSEQUENCE OF WELDING
Residual Stresses. 1987;39-58   Crossref logo
Link1 Link2

Fatigue surface crack propagation and intersecting cracks in connection with welding residual stresses
Fatigue & Fracture of Engineering Materials & Structures. 2018;   Crossref logo
Link1 Link2

On Welding Residual Stresses Near Fatigue Crack Tips
Advanced Materials Research. 2014;996:801-807   Crossref logo
Link1

Crack path predictions in anisotropic structures considering residual stresses
PAMM. 2017;17(1):247-248   Crossref logo
Link1 Link2

Effect of welding conditions on residual stresses due to butt welds
International Journal of Pressure Vessels and Piping. 1998;75(12):857-864   Crossref logo
Link1 Link2

Laser shock peening induced residual stresses and the effect on crack propagation behavior
International Journal of Fatigue. 2017;100:407-417   Crossref logo
Link1 Link2