Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effects of Electrode Face Radius and Force on Resistance Spot Weldability of Aluminium Alloy 6061
Hyeong-geun Jo, Young-Min Kim, Moon-Jin Kang, Dong-Cheol Kim
JWJ. 2018;36(6):46-51.   Published online 2018 November 26    DOI: https://doi.org/10.5781/JWJ.2018.36.6.8

Excel Download

Effects of Electrode Face Radius and Force on Resistance Spot Weldability of Aluminium Alloy 6061
Journal of Welding and Joining. 2018;36(6):46-51   Crossref logo
Link1 Link2 Link3

The Effects of Electrode Force on the Mechanical Behaviour of Resistance Spot-Welded 5083-O Aluminium Alloy Joints
Strain. 2009;47:e196-e204   Crossref logo
Link1

The effects of aging on machinability of 6061 aluminium alloy
Materials & Design. 2009;30(5):1480-1483   Crossref logo
Link1 Link2

Effects of alumina fibre content on properties of a PM aluminium alloy 6061
Metal Powder Report. 1992;47(3):62   Crossref logo
Link1 Link2

Resistance spot weldability and high cycle fatigue behaviour of martensitic (M190) steel sheet
Fatigue & Fracture of Engineering Materials & Structures. 2010;34(1):46-52   Crossref logo
Link1

The fracture of boron fibrereinforced 6061 aluminium alloy
Composites. 1979;10(4):243   Crossref logo
Link1 Link2

Welding parameters influence on fatigue life and microstructure in resistance spot welding of 6061-T6 aluminum alloy
Materials & Design. 2013;45:456-465   Crossref logo
Link1 Link2

Coating effects on contact conditions in resistance spot weldability
Journal of Materials Processing Technology. 2018;253:160-167   Crossref logo
Link1 Link2

Resistance Spot Weldability of Galvanize Coated and Uncoated TRIP Steels
Metals. 2016;6(12):299   Crossref logo
Link1

Resistance Spot Welding of 7075 Aluminium Alloy
Vehicle and Automotive Engineering 2. 2018;679-693   Crossref logo
Link1

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.