Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
A Study on the Characteristics of Laser Cladding Using the LC-190 Cemented Carbide Powder(II) - Characteristic Analysis of Multi-pass Clad Layer -
Jong-Do Kim, Su-Han Park, Moo-Keun Song
JWJ. 2018;36(6):40-45.   Published online 2018 November 26    DOI: https://doi.org/10.5781/JWJ.2018.36.6.7

Excel Download

A Study on the Characteristics of Laser Cladding Using the LC-190 Cemented Carbide Powder(II) - Characteristic Analysis of Multi-pass Clad Layer -
Journal of Welding and Joining. 2018;36(6):40-45   Crossref logo
Link1 Link2 Link3

A Study on the Characteristics of Laser Cladding Using the LC-190 Cemented Carbide Powder(I) - Characteristic Analysis of One-pass Clad Layer with Parameters -
Journal of Welding and Joining. 2018;36(6):34-39   Crossref logo
Link1 Link2 Link3

Characteristic behaviours of clad layer by a multi-layer laser cladding with powder mixture of Stellite-6 and tungsten carbide
Surface and Coatings Technology. 2006;201(6):3385-3392   Crossref logo
Link1 Link2

Machining tests on multi-layer coated cemented carbide cutting tools
Metal Powder Report. 1997;52(12):45   Crossref logo
Link1 Link2

Problems of spontaneous cubic carbide layer formation on cemented carbide free surfaces
Metal Powder Report. 1996;51(7):44   Crossref logo
Link1 Link2

Study on cross-section clad profile in coaxial single-pass cladding with a low-power laser
Optics & Laser Technology. 2005;37(6):478-482   Crossref logo
Link1 Link2

Predicting the geometric form of clad in laser cladding by powder using multiple regression analysis (MRA)
Materials & Design. 2008;29(2):554-557   Crossref logo
Link1 Link2

Prediction of clad angle in laser cladding by powder using response surface methodology and scatter search
Optics & Laser Technology. 2007;39(6):1130-1134   Crossref logo
Link1 Link2

Machining of austenitic stainless steels using CVD multi-layer coated cemented carbide tools
Tribology International. 2006;39(6):565-569   Crossref logo
Link1 Link2

Cemented carbide reinforced nickel-based alloy coating by laser cladding and the wear characteristics
Materials & Design. 1996;17(5-6):289-296   Crossref logo
Link1 Link2