Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Influence of Workpiece Tilting Angle on Joint Properties in Tailor Friction Stir Welded Blanks of Aluminium Alloy 5052-H32
Chan-Seung Ro, Hee-Seon Bang, Han-Sur Bang, Seung-Ji Yoo, Jong-Hee Kim, Eun-Gyeol Choi
JWJ. 2018;36(5):39-44.   Published online 2018 September 17    DOI: https://doi.org/10.5781/JWJ.2018.36.5.5

Excel Download

Influence of Workpiece Tilting Angle on Joint Properties in Tailor Friction Stir Welded Blanks of Aluminium Alloy 5052-H32
Journal of Welding and Joining. 2018;36(5):39-44   Crossref logo
Link1 Link2 Link3

Quality Prediction Of Friction Stir Weld Joints On AA 5052 H32 Aluminium Alloy Using Fuzzy Logic Technique
Materials Today: Proceedings. 2018;5(5):12124-12132   Crossref logo
Link1 Link2

Lightweight metal alloy tailor welded blanks
Tailor Welded Blanks for Advanced Manufacturing. 2011;97-117   Crossref logo
Link1 Link2 Link3

Establishing Mathematical Relationships to Study Tensile Behavior of Friction Stir Welded AA5086-H32 Aluminium Alloy Joints
Silicon. 2018;11(1):51-65   Crossref logo
Link1 Link2 Link3

An Etching Technique for Characterizing Friction Stir Welds in Aluminum Alloy Tailor Welded Blanks
Metallography, Microstructure, and Analysis. 2018;7(5):630-634   Crossref logo
Link1 Link2 Link3

Mechanical properties and microstructure of friction stir welded tailor-made blanks
Materials Science and Engineering: A. 2008;494(1-2):281-290   Crossref logo
Link1 Link2

Mechanical behaviour of dissimilar friction stir welded tailor welded blanks in Al–Mg alloys for Marine applications
Materials & Design. 2014;59:323-332   Crossref logo
Link1 Link2

Weld integrity of tailor welded blanks
Tailor Welded Blanks for Advanced Manufacturing. 2011;3-23   Crossref logo
Link1 Link2 Link3

Tailor welded blanks for the automotive industry
Tailor Welded Blanks for Advanced Manufacturing. 2011;164-180   Crossref logo
Link1 Link2 Link3

Microstructure and microtextural studies of friction stir welded aluminium alloy 5052
Materials & Design. 2011;32(3):1657-1666   Crossref logo
Link1 Link2