Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Laser and Gas Metal Arc Based Dissimilar Joining of Automotive Aluminium Alloys and Steel Sheets - A Review
Atanu Das, Hee-Seon Bang
JWJ. 2018;36(5):1-11.   Published online 2018 October 26    DOI: https://doi.org/10.5781/JWJ.2018.36.5.1

Excel Download

Laser and Gas Metal Arc Based Dissimilar Joining of Automotive Aluminium Alloys and Steel Sheets - A Review
Journal of Welding and Joining. 2018;36(5):1-11   Crossref logo
Link1 Link2 Link3

Gas Metal Arc Lap Joining of Aluminium Alloys and Steel Sheets
Journal of Welding and Joining. 2018;36(5):19-26   Crossref logo
Link1 Link2 Link3

Lichtbogenfügen umformbarer Stahl-Aluminium-Mischverbindungen. Arc joining of ductile steel-aluminium-dissimilar-metal-welds
Materialwissenschaft und Werkstofftechnik. 2010;41(11):951-960   Crossref logo
Link1

A Study on the Dissimilar Metal Joining of Aluminum to Steel Using the Arc Heat Source (Ⅱ) - Mechanism of Dissimilar Metal Joining -
Journal of Welding and Joining. 2018;36(4):13-22   Crossref logo
Link1 Link2 Link3

Dissimilar gas tungsten arc weld-brazing of Al/steel using Al-Si filler metal: Microstructure and strengthening mechanisms
Journal of Alloys and Compounds. 2018;749:121-127   Crossref logo
Link1 Link2

Joining of aluminium alloy and galvanized steel using a controlled gas metal arc process
Journal of Manufacturing Processes. 2017;27:179-187   Crossref logo
Link1 Link2

Microstructure reaction control of dissimilar automotive aluminium to galvanized steel sheets ultrasonic spot welding
Materials Science and Engineering: A. 2016;678:72-84   Crossref logo
Link1 Link2

Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel
Journal of Welding and Joining. 2017;35(5):16-22   Crossref logo
Link1 Link2 Link3

Gas-tungsten arc welding of magnesium alloys
Welding and Joining of Magnesium Alloys. 2010;160-177   Crossref logo
Link1 Link2 Link3

Hybrid laser-arc welding of magnesium alloys
Welding and Joining of Magnesium Alloys. 2010;229-253e   Crossref logo
Link1 Link2 Link3

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.