Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Study on Diffusion Bonding Characteristics of Austenitic Stainless Steels
Ho-Shin Jeong, Kook-Soo Bang
JWJ. 2018;36(5):81-87.   Published online 2018 October 26    DOI: https://doi.org/10.5781/JWJ.2018.36.5.11

Excel Download

Study on Diffusion Bonding Characteristics of Austenitic Stainless Steels
Journal of Welding and Joining. 2018;36(5):81-87   Crossref logo
Link1 Link2 Link3

Introduction to Austenitic Stainless Steels
Corrosion of Austenitic Stainless Steels. 2002;1-36   Crossref logo
Link1 Link2 Link3

High Temperature Corrosion of Austenitic Stainless Steels
Corrosion of Austenitic Stainless Steels. 2002;265-286   Crossref logo
Link1 Link2 Link3

Study of Fracture Mechanisms at Cyclic Fatigue of Austenitic Steels Used in Nuclear Reactors
Austenitic Stainless Steels - New Aspects. 2017;   Crossref logo
Link1

Introductory Chapter: Why Austenitic Stainless Steels are Continuously Interesting for Science?
Austenitic Stainless Steels - New Aspects. 2017;   Crossref logo
Link1

Considerations in the Design of Formable Austenitic Stainless Steels Based on Deformation-Induced Processes
Austenitic Stainless Steels - New Aspects. 2017;   Crossref logo
Link1

Surface Modification for Corrosion Protection of Austenitic Stainless Steels
Corrosion of Austenitic Stainless Steels. 2002;340-362   Crossref logo
Link1 Link2 Link3

Uniform Corrosion of Austenitic Stainless Steels
Corrosion of Austenitic Stainless Steels. 2002;37-73   Crossref logo
Link1 Link2 Link3

Pitting Corrosion of Austenitic Stainless Steels and Their Weldments
Corrosion of Austenitic Stainless Steels. 2002;74-105   Crossref logo
Link1 Link2 Link3

Friction Welding of Austenitic Stainless Steel with Copper Material
Austenitic Stainless Steels - New Aspects. 2017;   Crossref logo
Link1

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.