Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Anticorrosion Performance of FCAW Cladding with Regard to the Influence of Heat Input
Manas Kumar Saha, Ajit Mondal, Ritesh Hazra, Santanu Das
JWJ. 2018;36(5):61-69.   Published online 2018 October 10    DOI: https://doi.org/10.5781/JWJ.2018.36.5.8

Excel Download

Anticorrosion Performance of FCAW Cladding with Regard to the Influence of Heat Input
Journal of Welding and Joining. 2018;36(5):61-69   Crossref logo
Link1 Link2 Link3

Effect of FCAW Process Parameters on Weld Bead Geometry in Stainless Steel Cladding
Journal of Minerals and Materials Characterization and Engineering. 2011;10(09):827-842   Crossref logo
Link1 Link2

Effect of Heat Input on Stellite 6 Coatings on a Medium Carbon Steel Substrate by Laser Cladding
Materials Today: Proceedings. 2015;2(4-5):1747-1754   Crossref logo
Link1 Link2

The influence of wall thickness, thermal conductivity and method of heat input on the heat transfer performance of some ribbed surfaces
International Journal of Heat and Mass Transfer. 1972;15(5):1159-1169   Crossref logo
Link1 Link2

Performance of a dehumidifying compression heat pump with auxiliary heat input
Heat Recovery Systems and CHP. 1992;12(3):211-223   Crossref logo
Link1 Link2

The thermal performance of heat pipes with localized heat input
International Journal of Heat and Mass Transfer. 1989;32(7):1279-1287   Crossref logo
Link1 Link2

Heat input and metal transfer influences on the weld geometry and microstructure during underwater wet FCAW
Journal of Materials Processing Technology. 2016;238:373-382   Crossref logo
Link1 Link2

Influence of Residual Stress Caused by Cladding of Anticorrosion Layer in Nozzle Zone of RPV WWER-1000 on Results of Brittle Strength Evaluation
Proceedings of the First International Conference on Theoretical, Applied and Experimental Mechanics. 2018;409-411   Crossref logo
Link1

Inner cladding influence on mode interaction in symmetry-free photonic crystal fibers under heat load
Optical and Quantum Electronics. 2017;49(10):   Crossref logo
Link1 Link2 Link3

Effect of finite heat input on the power performance of micro heat engines
Energy. 2011;36(5):2686-2692   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.