Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Welding Residual Stress Evaluation and Process Optimization of CTBA Trailing Arm using Finite Element Analysis
Jong-sung Kim, In-hyeok Im, Jung-sub Kim, Jung-sik Suh
JWJ. 2018;36(4):70-74.   Published online 2018 August 6    DOI: https://doi.org/10.5781/JWJ.2018.36.4.8

Excel Download

Welding Residual Stress Evaluation and Process Optimization of CTBA Trailing Arm using Finite Element Analysis
Journal of Welding and Joining. 2018;36(4):70-74   Crossref logo
Link1 Link2 Link3

Finite element modeling of laser beam welding for residual stress calculation
PAMM. 2017;17(1):415-416   Crossref logo
Link1 Link2

Evaluation of Parametric Significance in Friction Welding Process of AA1100 and Zr705 Alloy using Finite Element Analysis
Materials Today: Proceedings. 2017;4(2):2624-2631   Crossref logo
Link1 Link2

Residual stress evaluation in resin-molded IC chips using finite element analysis and piezoresistive gauges
Microelectronics Reliability. 2008;48(6):923-932   Crossref logo
Link1 Link2

Using finite element and ultrasonic method to evaluate welding longitudinal residual stress through the thickness in austenitic stainless steel plates
Materials & Design. 2013;45:628-642   Crossref logo
Link1 Link2

Residual stress analysis and finite element modelling of repair-welded titanium sheets
Welding in the World. 2017;61(6):1211-1223   Crossref logo
Link1 Link2 Link3

Finite element analysis of residual stress induced by shot peening process
Advances in Engineering Software. 2003;34(9):569-575   Crossref logo
Link1 Link2

Thermal Stress Analysis of dissimilar welding joints by Finite Element Method
Procedia Engineering. 2011;15:3860-3864   Crossref logo
Link1 Link2

Finite Element Modelling of Welding Residual Stress and Its Influence on Creep Behavior of a 2.25Cr-1Mo-0.25V Steel Cylinder
Procedia Engineering. 2015;130:552-559   Crossref logo
Link1 Link2

Some studies on weld bead geometries for laser spot welding process using finite element analysis
Materials & Design. 2012;34:412-426   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.