Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Corrosion Properties and Failure Behavior of Al/Fe Self-Piercing Rivet Joint
Sanghoon Kang, Jin Young Yoon, Cheolhee Kim
JWJ. 2018;36(3):72-77.   Published online 2018 June 25    DOI: https://doi.org/10.5781/JWJ.2018.36.3.11

Excel Download

Corrosion Properties and Failure Behavior of Al/Fe Self-Piercing Rivet Joint
Journal of Welding and Joining. 2018;36(3):72-77   Crossref logo
Link1 Link2 Link3

Long-term Corrosion Studies of a CFRP/EN AW-6060-T6 Self-piercing rivet Joint and a Steel/EN AW-6060-T6 Blind Rivet Joint
Materials Today: Proceedings. 2015;2:S131-S140   Crossref logo
Link1 Link2

Long-term corrosion behaviour of EN AW-6060-T6 in an aluminium/carbon-fibre reinforced polymer self-piercing rivet joint
Materialwissenschaft und Werkstofftechnik. 2014;45(12):1123-1129   Crossref logo
Link1 Link2

Correlation between microstructure and corrosion behavior of two Al-Fe-Si alloys
Materials and Corrosion. 2015;67(3):286-296   Crossref logo
Link1

The failure mechanics analysis of the solid self-piercing riveting joints
Engineering Failure Analysis. 2015;47:77-88   Crossref logo
Link1 Link2

Neutral salt spray tests on Fe–Al and Fe–Al–X
Corrosion Science. 2012;64:74-81   Crossref logo
Link1 Link2

Mechanical properties and oxidation—corrosion behavior of AlN-coated Fe-Al-Mn alloys
Surface and Coatings Technology. 1992;56(1):61-70   Crossref logo
Link1 Link2

Effect of sintering temperature on the corrosion properties of nanostructured Fe-18Cr-2Si alloy prepared by SPS
Materials and Corrosion. 2016;68(3):361-367   Crossref logo
Link1 Link2

Influence of cooling rate on the microstructure and corrosion behavior of Al–Fe alloys
Corrosion Science. 2015;100:396-403   Crossref logo
Link1 Link2

Oxidation of Fe–Si, Fe–Al and Fe–Si–Al alloys in CO2–H2O gas at 800°C
Corrosion Science. 2012;54:127-138   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.