Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Resistance Spot Welding Characteristic of 1500MPa Steel Sheet Using Simulation (I) - Lobe Curve Characteristic Analysis of Resistance Spot Welding -
Jong-Jung Lee, Chang-soek Son, Young Whan Park
JWJ. 2018;36(3):45-50.   Published online 2018 June 20    DOI: https://doi.org/10.5781/JWJ.2018.36.3.7

Excel Download

Resistance Spot Welding Characteristic of 1500MPa Steel Sheet Using Simulation (I) - Lobe Curve Characteristic Analysis of Resistance Spot Welding -
Journal of Welding and Joining. 2018;36(3):45-50   Crossref logo
Link1 Link2 Link3

Resistance Spot Welding Characteristic of 1500MPa Steel Sheet Using Simulation (II) - Estimation Model for Nugget Diameter of Resistance Spot Welds -
Journal of Welding and Joining. 2018;36(3):51-56   Crossref logo
Link1 Link2 Link3

Resistance spot weldability and high cycle fatigue behaviour of martensitic (M190) steel sheet
Fatigue & Fracture of Engineering Materials & Structures. 2010;34(1):46-52   Crossref logo
Link1

Experimental investigation and numerical simulation of resistance spot welding for residual stress evaluation of DP1000 steel
Welding in the World. 2016;60(3):393-402   Crossref logo
Link1 Link2 Link3

Optimization of Welding Parameters in Resistance Spot Welding of 980 MPa Grade GA Steel Sheet using Multi-Response Surface Methodology
Journal of Welding and Joining. 2018;36(4):63-69   Crossref logo
Link1 Link2 Link3

Regression modeling and process analysis of resistance spot welding on galvanized steel sheet
Materials & Design. 2009;30(7):2547-2555   Crossref logo
Link1 Link2

Strength prediction of sheet to tube single sided resistance spot welding
Materials & Design. 2009;30(10):4328-4334   Crossref logo
Link1 Link2

Optimization of resistance spot welding parameters for microalloyed steel sheets
Open Engineering. 2016;6(1):   Crossref logo
Link1 Link2

Ultrasonic Spot Welding of Nickel Foam Sheet and Aluminum Solid Sheet  
Advanced Engineering Materials. 2017;19(8):1700094   Crossref logo
Link1 Link2

Effect of cover sheet on dissimilar three-steel sheets resistance spot welding
The International Journal of Advanced Manufacturing Technology. 2016;89(1-4):483-491   Crossref logo
Link1 Link2 Link3 Link4