Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
A Study on the Electrochemical Corrosion Property of Sn-xSb Solder Alloy
Junhyuk Son, Dong-Yurl Yu, Yong-Ho Ko, Junghwan Bang
JWJ. 2018;36(3):78-82.   Published online 2018 June 19    DOI: https://doi.org/10.5781/JWJ.2018.36.3.12

Excel Download

A Study on the Electrochemical Corrosion Property of Sn-xSb Solder Alloy
Journal of Welding and Joining. 2018;36(3):78-82   Crossref logo
Link1 Link2 Link3

Electrochemical corrosion study of Sn–3Ag–3Cu solder alloy in NaCl solution
Electrochimica Acta. 2009;54(28):7231-7235   Crossref logo
Link1 Link2

Effect of trace Mn modification on the microstructure and corrosion behavior of Sn−9Zn solder alloy
Materials and Corrosion. 2017;69(6):781-792   Crossref logo
Link1 Link2

Fracture of sustained tensile-loaded Sn–3.0Ag–0.5Cu solder alloy in NaCl solution
Corrosion Science. 2011;53(10):3331-3336   Crossref logo
Link1 Link2

Electrochemical corrosion behaviour of Sn-Ag-Cu (SAC) eutectic alloy in a chloride containing environment
Materials and Corrosion. 2011;n/a-n/a   Crossref logo
Link1

Creep corrosion cracking of Sn–3.0Ag and Sn–0.5Cu solder alloys in NaCl solution
Corrosion Science. 2014;86:142-148   Crossref logo
Link1 Link2

Improvement of wettability and tensile property in Sn–Ag–RE lead-free solder alloy
Materials Letters. 2002;56(6):1039-1042   Crossref logo
Link1 Link2

Effect of Antimony Additions on Corrosion and Mechanical Properties of Sn-Bi Eutectic Lead-Free Solder Alloy
Materials Sciences and Applications. 2012;03(06):355-362   Crossref logo
Link1 Link2 Link3

Corrosion Behavior of Corroded Sn–3.0Ag–0.5Cu Solder Alloy
Procedia Chemistry. 2016;19:847-854   Crossref logo
Link1 Link2

Microstructure, corrosion behaviour and microhardness of a directionally solidified Sn–Cu solder alloy
Electrochimica Acta. 2011;56(24):8891-8899   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.