Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Parametric Study of Self-Piercing Riveting for CFRP-Aluminum Dissimilar Joint
Nam-Ki Jeon, Sehun Rhee, Dong-Hyuck Kam
JWJ. 2018;36(3):8-17.   Published online 2018 June 4    DOI: https://doi.org/10.5781/JWJ.2018.36.3.2

Excel Download

Parametric Study of Self-Piercing Riveting for CFRP-Aluminum Dissimilar Joint
Journal of Welding and Joining. 2018;36(3):8-17   Crossref logo
Link1 Link2 Link3

Joining of Lightweight Dissimilar Materials by Friction Self-Piercing Riveting
Frontiers in Geotechnical Engineering. 2019;189-195   Crossref logo
Link1

Friction Self-Piercing Riveting (F-SPR) of Dissimilar Materials
Procedia Engineering. 2017;207:950-955   Crossref logo
Link1 Link2

Self-piercing riveting of similar and dissimilar metal sheets of aluminum alloy and copper alloy
Materials & Design (1980-2015). 2015;65:923-933   Crossref logo
Link1 Link2

Fatigue of Aluminum/Glass Fiber Reinforced Polymer Composite Assembly Joined by Self-piercing Riveting
Procedia Engineering. 2015;133:501-507   Crossref logo
Link1 Link2

Self-piercing riveting of aluminum alloy and thermoplastic composites
Journal of Composite Materials. 2014;49(12):1493-1502   Crossref logo
Link1 Link2 Link3

Durability on alternate immersion test of self-piercing riveting aluminium joint
Materials & Design. 2013;46:849-856   Crossref logo
Link1 Link2

The failure mechanics analysis of the solid self-piercing riveting joints
Engineering Failure Analysis. 2015;47:77-88   Crossref logo
Link1 Link2

Thermo-mechanical modelling and finite element analysis of self-piercing riveting processes
PAMM. 2018;18(1):e201800234   Crossref logo
Link1 Link2

Experimental and numerical appraisal of self-piercing riveting
CIRP Annals. 2009;58(1):17-20   Crossref logo
Link1 Link2