Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Characteristics of Sulfide Stress Cracking of High Strength Pipeline Steel Weld by Heat Input
Byoung-Hyun Yoon
JWJ. 2018;36(3):38-44.   Published online 2018 May 29    DOI: https://doi.org/10.5781/JWJ.2018.36.3.6

Excel Download

Characteristics of Sulfide Stress Cracking of High Strength Pipeline Steel Weld by Heat Input
Journal of Welding and Joining. 2018;36(3):38-44   Crossref logo
Link1 Link2 Link3

Effect of heat input and preheating on hydrogen assisted weld joint cracking of a 0.13% C, 1.5% Mn, 0.032% Nb high strength steel of 50 mm plate thickness in the IRC test
Steel Research. 1987;58(12):570-576   Crossref logo
Link1 Link2 Link3

Effect of post weld heat treatment on stress corrosion cracking of a low alloy steel to stainless steel transition weld
Corrosion Science. 2001;43(10):1963-1983   Crossref logo
Link1 Link2

Cracking in high performance superduplex stainless steel welds
Weld Cracking in Ferrous Alloys. 2009;353-392   Crossref logo
Link1 Link2 Link3

Influence of carbon on stress corrosion cracking of high strength pipeline steel
Corrosion Science. 2013;76:486-493   Crossref logo
Link1 Link2

Sulfide stress cracking resistance of API-X100 high strength low alloy steel
Materials & Design. 2009;30(10):4088-4094   Crossref logo
Link1 Link2

A study on cold cracking susceptibility in high strength steel fillet weld joints
Steel Research. 1994;65(12):551-555   Crossref logo
Link1 Link2 Link3

Welding stress control in high-strength steel components using adapted heat control concepts
Welding in the World. 2018;   Crossref logo
Link1 Link2 Link3

Cold work effects on sulfide stress cracking of pipeline steel exposed to sour environments
Corrosion Science. 1993;34(1):61-78   Crossref logo
Link1 Link2

The caustic stress corrosion cracking of high-strength steel wire
Corrosion Science. 1981;21(6):409-415   Crossref logo
Link1 Link2