Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of Composition on Strain-Induced Martensite Transformation and Tensile Stress-Strain Curve for Austenitic Stainless Steels
Ju Hyun Noh, Sang Gwon Lee, Hanji Park, Namhyun Kang
JWJ. 2018;36(2):28-33.   Published online 2018 April 30    DOI: https://doi.org/10.5781/JWJ.2018.36.2.5

Excel Download

Effect of Composition on Strain-Induced Martensite Transformation and Tensile Stress-Strain Curve for Austenitic Stainless Steels
Journal of Welding and Joining. 2018;36(2):28-33   Crossref logo
Link1 Link2 Link3

Strain aging behavior of austenitic stainless steels containing strain induced martensite
Scripta Materialia. 2000;42(9):887-891   Crossref logo
Link1 Link2

Strain induced martensite formation and its effect on strain hardening behavior in the cold drawn 304 austenitic stainless steels
Scripta Materialia. 1997;36(1):99-104   Crossref logo
Link1 Link2

Strain hardening and transformation mechanism of deformation-induced martensite transformation in metastable austenitic stainless steels
Materials Science and Engineering: A. 1991;141(2):189-198   Crossref logo
Link1 Link2

Characterisation of strain-induced martensite in a metastable austenitic stainless steel by nanoindentation
Strain. 2010;47:129-133   Crossref logo
Link1

Effect of strain-induced martensite on hydrogen environment embrittlement of sensitized austenitic stainless steels at low temperatures
Acta Materialia. 1998;46(13):4559-4570   Crossref logo
Link1 Link2

Formation of shear bands and strain-induced martensite during plastic deformation of metastable austenitic stainless steels
Acta Materialia. 2007;55(18):6108-6118   Crossref logo
Link1 Link2

ANN modeling of strain-induced martensite and its applications in metastable austenitic stainless steels
Journal of Alloys and Compounds. 2009;476(1-2):352-355   Crossref logo
Link1 Link2

Influence of strain-induced martensite in the anodic dissolution of austenitic stainless steels in acid medium
Corrosion Science. 2013;69:130-138   Crossref logo
Link1 Link2

Modelling kinetics of strain-induced martensite transformation during plastic deformation of austenitic stainless steel
Materials & Design. 2016;109:466-475   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.