Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of Post-Weld Heat Treatment Temperature on the Mechanical Properties and Microstructure of Simulated Weld Heat-Affected Zone of SA-516 Grade 70 Carbon Steel
So-Young Park, Yongjoon Kang, Sung-Sik Kang, Seung-Gun Lee
JWJ. 2018;36(2):82-88.   Published online 2018 April 26    DOI: https://doi.org/10.5781/JWJ.2018.36.2.12

Excel Download

Effect of Post-Weld Heat Treatment Temperature on the Mechanical Properties and Microstructure of Simulated Weld Heat-Affected Zone of SA-516 Grade 70 Carbon Steel
Journal of Welding and Joining. 2018;36(2):82-88   Crossref logo
Link1 Link2 Link3

Effect of post weld heat treatment and heat input on the microstructure and mechanical properties of plasma arc welded AISI 410S ferritic stainless steel
Materials Research Express. 2019;6(6):066517   Crossref logo
Link1 Link2 Link3 Link4 Link5 Link6 Link7 Link8

THE EFFECT OF HEAT TREATMENT ON THE MICROSTRUCTURE AND PROPERTIES OF STRUCTURAL STEEL WELD DEPOSITS
Welding for Challenging Environments. 1986;263-272   Crossref logo
Link1 Link2

Effect of Post-weld Heat Treatment on Microstructure and Mechanical Properties of 309L/E5015 Fusion Zone of Bimetal Lined Pipe Weld
Advances in Materials Processing. 2018;435-444   Crossref logo
Link1

Dynamic fracture behaviour of simulated weld heat affected zone of a high strength low alloy steel
Steel Research. 1996;67(12):555-557   Crossref logo
Link1 Link2 Link3

Effect of post weld heat treatment on steel plate deck with trough rib by portable heat source
Welding in the World. 2017;61(6):1225-1235   Crossref logo
Link1 Link2 Link3

Effect of Weld Thermal Cycles on Microstructures and Mechanical Properties in Simulated Heat Affected Zone of a HY 85 Steel
Transactions of the Indian Institute of Metals. 2016;70(1):239-250   Crossref logo
Link1 Link2 Link3 Link4

Effect of weld thermal cycle on microstructure and fracture toughness of simulated heat-affected zone for a 800MPa grade high strength low alloy steel
Journal of Materials Processing Technology. 2008;207(1-3):30-39   Crossref logo
Link1 Link2

Effect of Groove Design and Post-Weld Heat Treatment on Microstructure and Mechanical Properties of P91 Steel Weld
Journal of Materials Engineering and Performance. 2016;25(7):2761-2775   Crossref logo
Link1 Link2 Link3

Characterization on the Microstructure Evolution and Toughness of TIG Weld Metal of 25Cr2Ni2MoV Steel after Post Weld Heat Treatment
Metals. 2018;8(3):160   Crossref logo