Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Experimental and Numerical Study on Effect of Weld Reinforcement on Angular Distortion of SAW Square Butt Welded Plates
H. K. Narang, M. M. Mahapatra, P. K. Jha, PVSS Sridhar, P. Biswas
JWJ. 2018;36(2):48-59.   Published online 2018 April 2    DOI: https://doi.org/10.5781/JWJ.2018.36.2.8

Excel Download

Experimental and Numerical Study on Effect of Weld Reinforcement on Angular Distortion of SAW Square Butt Welded Plates
Journal of Welding and Joining. 2018;36(2):48-59   Crossref logo
Link1 Link2 Link3

The Effect of Weld Reinforcement and Post-Welding Cooling Cycles on Fatigue Strength of Butt-Welded Joints under Cyclic Tensile Loading
Materials. 2018;11(4):594   Crossref logo
Link1

Finite Element Analysis of Heat Input Effect on Temperature, Residual Stresses and Distortion in Butt Welded Plates
Materials Today: Proceedings. 2018;5(2):8328-8337   Crossref logo
Link1 Link2

Experimental and Numerical Results
Soil Reinforcement for Anchor Plates and Uplift Response. 2017;97-143   Crossref logo
Link1 Link2

Prediction of welding-induced angular distortions in thin butt-welded plates using artificial neural networks
Computational Materials Science. 2012;62:152-159   Crossref logo
Link1 Link2

The multiaxial weld root fatigue of butt welded joints subjected to uniaxial loading
Fatigue & Fracture of Engineering Materials & Structures. 2016;39(10):1281-1298   Crossref logo
Link1

Experimental and numerical study of thermal field and weld bead characteristics in submerged arc welded plate
Journal of Materials Processing Technology. 2017;248:262-274   Crossref logo
Link1 Link2

Numerical Simulation and Artificial Neural Network Modeling for Predicting Welding-Induced Distortion in Butt-Welded 304L Stainless Steel Plates
Metallurgical and Materials Transactions B. 2015;47(1):702-713   Crossref logo
Link1 Link2 Link3

Effect of vibratory weld conditioning on the residual stresses and distortion in multipass girth-butt welded pipes
International Journal of Pressure Vessels and Piping. 2007;84(5):298-303   Crossref logo
Link1 Link2

Effect of reinforcement on fatigue strength of butt welded joints for aluminium alloyShinoda, T. and Masumoto, I. Kei Kinzoku Yosetsu (J. Light Met. Weld. Constr.) Nov. 1988 26, (11), 1–7 (in Japanese)
International Journal of Fatigue. 1989;11(4):282-282   Crossref logo
Link1 Link2