Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Study on the Fracture Toughness of FCA Weldment with the Yield Strength 420MPa Grade High Strength Steels for Offshore Structures Depending on the Welding Position
In-Chan Kim, Sang-Hoon Jeong, Han-Geul Choi, Myung-Hyun Kim
JWJ. 2018;36(2):67-73.   Published online 2018 April 2    DOI: https://doi.org/10.5781/JWJ.2018.36.2.10

Excel Download

Study on the Fracture Toughness of FCA Weldment with the Yield Strength 420MPa Grade High Strength Steels for Offshore Structures Depending on the Welding Position
Journal of Welding and Joining. 2018;36(2):67-73   Crossref logo
Link1 Link2 Link3

High-power beam welding of advanced high-strength steels (AHSS)
Welding and Joining of Advanced High Strength Steels (AHSS). 2015;93-119   Crossref logo
Link1 Link2

Laser welding of advanced high-strength steels (AHSS)
Welding and Joining of Advanced High Strength Steels (AHSS). 2015;71-92   Crossref logo
Link1 Link2

Resistance spot welding techniques for advanced high-strength steels∗ (AHSS)
Welding and Joining of Advanced High Strength Steels (AHSS). 2015;55-70   Crossref logo
Link1 Link2

Fracture toughness of 180 to 210 k.s.i. yield strength steels
Wear. 1970;16(1-2):162   Crossref logo
Link1 Link2

Use of Niobium High Strength Steels with 450 MPA Yield Strength for Construction
HSLA Steels 2015, Microalloying 2015 & Offshore Engineering Steels 2015. 2016;931-939   Crossref logo
Link1

Development of 690MPa High Strength Steel with Low Yield Ratio and Good Weldability for Building Structures in Wisco
HSLA Steels 2015, Microalloying 2015 & Offshore Engineering Steels 2015. 2016;459-466   Crossref logo
Link1

HIGH-STRENGTH, HIGH-FRACTURE TOUGHNESS SUBMERGED-ARC WELD FOR ARCTIC LINE PIPE
Welding for Challenging Environments. 1986;315-323   Crossref logo
Link1 Link2

Adhesive bonding techniques for advanced high-strength steels (AHSS)
Welding and Joining of Advanced High Strength Steels (AHSS). 2015;167-179   Crossref logo
Link1 Link2

Manufacturing of advanced high-strength steels (AHSS)
Welding and Joining of Advanced High Strength Steels (AHSS). 2015;29-53   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.