Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Study on the Corrosion Resistance of High Strength Bolt, Nut and Washer Set (S10T) Related to the Surface Treatment Conditions
Youn O Choi, Jung Woo Han, Hyun Seon Hong, Han Gil Suk
JWJ. 2018;36(2):34-39.   Published online 2018 March 8    DOI: https://doi.org/10.5781/JWJ.2018.36.2.6

Excel Download

Study on the Corrosion Resistance of High Strength Bolt, Nut and Washer Set (S10T) Related to the Surface Treatment Conditions
Journal of Welding and Joining. 2018;36(2):34-39   Crossref logo
Link1 Link2 Link3

On the applicability of high strength self-tapping aluminium bolts in magnesium nut materials for automotive applications
Materials and Corrosion. 2009;NA-NA   Crossref logo
Link1

Effect of alloying elements and surface treatment on corrosion fatigue strength of high-strength suspension coil springs
JSAE Review. 2001;22(3):337-342   Crossref logo
Link1 Link2

Looking for surface treatments with potential industrial use in high temperature oxidation conditions
Novel Approaches to Improving High Temperature Corrosion Resistance. 2008;264-275   Crossref logo
Link1 Link2 Link3

High nitrogen stainless steels with high strength and corrosion resistance
Metal Powder Report. 1997;51(1):35   Crossref logo
Link1 Link2

High nitrogen stainless steels with high strength and corrosion resistance
Metal Powder Report. 1997;52(1):35   Crossref logo
Link1 Link2

Axial force distributions on connection elements of the bolt-nut type
Strength of Materials. 1971;3(9):1103-1109   Crossref logo
Link1 Link2 Link3

Effect of surface pretreatment on corrosion resistance and bond strength of magnesium AZ31 alloy
Corrosion Science. 2013;66:33-42   Crossref logo
Link1 Link2

Silicon surface treatment via CVD of inner surface of steel pipes
Novel Approaches to Improving High Temperature Corrosion Resistance. 2008;236-248   Crossref logo
Link1 Link2 Link3

Enhanced corrosion resistance of high strength Mg–3Al–1Zn alloy sheets with ultrafine grains in a phosphate-buffered saline solution