Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Laser Cladding by Printing Si Powder Paste on A1050 Al Alloy Surface
Hyoung-Keun Lee
JWJ. 2018;36(1):57-64.   Published online 2018 January 26    DOI: https://doi.org/10.5781/JWJ.2018.36.1.7

Excel Download

Laser Cladding by Printing Si Powder Paste on A1050 Al Alloy Surface
Journal of Welding and Joining. 2018;36(1):57-64   Crossref logo
Link1 Link2 Link3

Laser Cladding with Al-36%Si Powder Paste on A319 Al Alloy Surface to Improve Wear Resistance
Journal of Welding and Joining. 2017;35(2):58-62   Crossref logo
Link1 Link2 Link3

Broad-beam laser cladding of Al–Si alloy coating on AZ91HP magnesium alloy
Surface and Coatings Technology. 2006;201(6):2701-2706   Crossref logo
Link1 Link2

Microstructure and corrosion resistance of magnesium alloy ZE41 with laser surface cladding by Al–Si powder
Surface and Coatings Technology. 2008;202(20):4901-4914   Crossref logo
Link1 Link2

Broad-beam laser cladding of Al–Cu alloy coating on AZ91HP magnesium alloy
Applied Surface Science. 2007;253(11):4917-4922   Crossref logo
Link1 Link2

Laser surface cladding of MRI 153M magnesium alloy with (Al+Al2O3)
Surface and Coatings Technology. 2009;203(16):2292-2299   Crossref logo
Link1 Link2

Composition design and laser cladding of Ni–Zr–Al alloy coating on the magnesium surface
Applied Surface Science. 2009;256(5):1609-1613   Crossref logo
Link1 Link2

Laser cladding of eutectic-based Ti–Ni–Al alloy coating on magnesium surface
Surface and Coatings Technology. 2010;205(1):189-194   Crossref logo
Link1 Link2

Laser Powder Cladding of Ti-6Al-4V α/β Alloy
Materials. 2017;10(10):1178   Crossref logo
Link1

YAG laser cladding of an Al-Si alloy onto an Mg/SiC composite for the improvement of corrosion resistance
Composites Science and Technology. 2001;61(11):1549-1554   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.