Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
The Effects of Nitrogen Content and Cold Rolling Reduction on the Mechanical Properties of New 420-series Stainless Steel Strip having a Mesh As-Welded Structure by the Electroslag Cladding
Jae-Young Jung
JWJ. 2017;35(6):42-50.   Published online 2017 December 31    DOI: https://doi.org/10.5781/JWJ.2017.35.6.7

Excel Download

The Effects of Nitrogen Content and Cold Rolling Reduction on the Mechanical Properties of New 420-series Stainless Steel Strip having a Mesh As-Welded Structure by the Electroslag Cladding
Journal of Welding and Joining. 2017;35(6):42-50   Crossref logo
Link1 Link2 Link3

Variations of Chemical Composition and Effects of Welding Parameters on the Overlay Welding Behaviors and Fluxes in Electroslag Cladding by using a New 420-series Stainless Steel Strip
Journal of Welding and Joining. 2017;35(6):32-41   Crossref logo
Link1 Link2 Link3

Electroslag and submerged arc stainless steel strip cladding
Anti-Corrosion Methods and Materials. 1998;45(1):41-47   Crossref logo
Link1 Link2

The Effects of Nitrogen Gas on Microstructural and Mechanical Properties of TIG Welded S32205 Duplex Stainless Steel
Metals. 2018;8(4):226   Crossref logo
Link1

Structure and properties of nitrogen stainless steel as a function of manganese content
Metal Powder Report. 1997;52(11):44   Crossref logo
Link1 Link2

Influence of nitrogen-induced grain refinement on mechanical properties of nitrogen alloyed type 316LN stainless steel
Journal of Nuclear Materials. 2012;420(1-3):473-478   Crossref logo
Link1 Link2

The Effect of Cold Rolling on Microstructure and Mechanical Properties of a New Cr–Mn Austenitic Stainless Steel in Comparison with AISI 316 Stainless Steel
Transactions of the Indian Institute of Metals. 2016;70(5):1251-1259   Crossref logo
Link1 Link2 Link3 Link4

Hybrid electroslag cladding (H-ESC): an innovation in high speed electroslag strip cladding
Welding in the World. 2019;   Crossref logo
Link1 Link2 Link3

Effects of Welding Parameters on the Overlay Welding Behaviors in Electroslag Cladding by using AISI 430 Stainless Steel Strip - Experimental Study
Journal of Welding and Joining. 2017;35(5):77-86   Crossref logo
Link1 Link2 Link3

The cold-rolling lubrication of steel strip
Wear. 1963;6(1):90   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.