Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
High Heat Input Electro-gas Arc Welding of TMCP Plate for Steel Storage Tanks
Kang-Mook Ryu, Dae-Woo Kim, Jin-Woo Lee, Hwan-Cheol Bang, Chul-Gyu Park, Hongchul Jeong
JWJ. 2017;35(6):27-31.   Published online 2017 December 26    DOI: https://doi.org/10.5781/JWJ.2017.35.6.5

Excel Download

High Heat Input Electro-gas Arc Welding of TMCP Plate for Steel Storage Tanks
Journal of Welding and Joining. 2017;35(6):27-31   Crossref logo
Link1 Link2 Link3

Development of High Heat Input Welding High Strength Steel Plate for Oil Storage Tank in Xinyu Steel Company
Energy Materials 2014. 2014;863-869   Crossref logo
Link1

The Development and Microstructure Analysis of High Strength Steel Plate NVE36 for Large Heat Input Welding
HSLA Steels 2015, Microalloying 2015 & Offshore Engineering Steels 2015. 2016;475-480   Crossref logo
Link1

Low heat input gas metal arc welding for dissimilar metal weld overlays part III: hydrogen-assisted cracking susceptibility
Welding in the World. 2019;   Crossref logo
Link1 Link2 Link3

Effect of Mg addition on formation of intragranular acicular ferrite in heat-affected zone of steel plate after high-heat-input welding
Journal of Iron and Steel Research International. 2018;25(4):433-441   Crossref logo
Link1 Link2 Link3

Development of High Heat Input Welding Offshore Steel as Normalized Condition
HSLA Steels 2015, Microalloying 2015 & Offshore Engineering Steels 2015. 2016;503-507   Crossref logo
Link1

SUBMERGED ARC WELDING OF HIGH YIELD STRENGTH STEEL
Welding for Challenging Environments. 1986;283-291   Crossref logo
Link1 Link2

The influence of welding heat input on submerged arc welded duplex steel joints imperfections
Journal of Materials Processing Technology. 2005;164-165:1082-1088   Crossref logo
Link1 Link2

Improvement of HAZ Toughness of Steel Plate for High Heat Input Welding by Inclusion Control with Mg Deoxidation
steel research international. 2015;86(6):619-625   Crossref logo
Link1

Effects of shielding gas composition on the welding stability, microstructure and mechanical properties in laser-arc hybrid welding of high nitrogen steel
Materials Research Express. 2018;5(9):096513   Crossref logo
Link1 Link2 Link3 Link4 Link5 Link6 Link7 Link8