Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Microstructure and Mechanical Properties of Reheated Zones in the Multi-pass Weld Metal of High-Strength Steel
Yongjoon Kang, Gitae Park, Seonghoon Jeong, Changhee Lee
JWJ. 2017;35(6):21-26.   Published online 2017 December 21    DOI: https://doi.org/10.5781/JWJ.2017.35.6.4

Excel Download

Microstructure and Mechanical Properties of Reheated Zones in the Multi-pass Weld Metal of High-Strength Steel
Journal of Welding and Joining. 2017;35(6):21-26   Crossref logo
Link1 Link2 Link3

Correlation Between Microstructure and Low-Temperature Impact Toughness of Simulated Reheated Zones in the Multi-pass Weld Metal of High-Strength Steel
Metallurgical and Materials Transactions A. 2017;49(1):177-186   Crossref logo
Link1 Link2 Link3

Influence of welding pass on microstructure and toughness in the reheated zone of multi-pass weld metal of 550 MPa offshore engineering steel
Materials Science and Engineering: A. 2017;702:196-205   Crossref logo
Link1 Link2

Effect of microstructure on mechanical properties in weld-repaired high strength low alloy steel
Materials & Design (1980-2015). 2012;36:233-242   Crossref logo
Link1 Link2

A Novel Low-Carbon High-Strength Steel: Processing, Microstructure and Mechanical Properties
Advanced High Strength Steel. 2018;125-133   Crossref logo
Link1

Influence of Y on microstructures and mechanical properties of high strength steel weld metal
Materials & Design (1980-2015). 2014;62:83-90   Crossref logo
Link1 Link2

Structure and mechanical properties of high temperature sintered high strength steel
Metal Powder Report. 1993;48(12):53   Crossref logo
Link1 Link2

Microstructure and mechanical properties of spray fromed high speed steel
Metal Powder Report. 1996;51(2):43   Crossref logo
Link1 Link2

Characterization of the Multi-Pass Weld Metal and the Effect of Post-Weld Heat Treatment on Its Microstructure and Toughness
HSLA Steels 2015, Microalloying 2015 & Offshore Engineering Steels 2015. 2016;481-488   Crossref logo
Link1

Effect of interpass temperature on the microstructure and mechanical properties of multi-pass weld metal in a 550-MPa-grade offshore engineering steel
Welding in the World. 2017;61(6):1155-1168   Crossref logo