Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
The Effect of PWHT on the Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW
Jun-Hyeok Hyun, Tae-Woo Shin, Bok-Su Jang, Sang-Ho Kim, Jin-Hyun Koh
JWJ. 2017;35(6):89-95.   Published online 2017 December 15    DOI: https://doi.org/10.5781/JWJ.2017.35.6.13

Excel Download

The Effect of PWHT on the Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW
Journal of Welding and Joining. 2017;35(6):89-95   Crossref logo
Link1 Link2 Link3

A Study on Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW
Journal of Welding and Joining. 2017;35(4):74-81   Crossref logo
Link1 Link2 Link3

A New Method to Recycle Stainless–Steel Duplex UNS S31803 Chips
Metals. 2018;8(7):546   Crossref logo
Link1

Effect of post-weld heat treatment on microstructure evolution and pitting corrosion behavior of UNS S31803 duplex stainless steel welds
Corrosion Science. 2012;62:42-50   Crossref logo
Link1 Link2

Effect of a brief post-weld heat treatment on the microstructure evolution and pitting corrosion of laser beam welded UNS S31803 duplex stainless steel
Corrosion Science. 2012;65:472-480   Crossref logo
Link1 Link2

The σ phase formation in annealed UNS S31803 duplex stainless steel: Texture aspects
Materials Characterization. 2008;59(9):1301-1306   Crossref logo
Link1 Link2

Influence of microstructure on the corrosion resistance of the duplex stainless steel UNS S31803
Materials Characterization. 2008;59(8):1127-1132   Crossref logo
Link1 Link2

Evaluation of Pitting Behavior on Solution Treated Duplex Stainless Steel UNS S31803
Journal of Materials Science & Technology. 2014;30(2):179-183   Crossref logo
Link1 Link2

WITHDRAWN: Improvement of the cavitation erosion resistance of UNS S31803 stainless steel by duplex treatment
Thin Solid Films. 2010;   Crossref logo
Link1 Link2

Improvement of the cavitation erosion resistance of UNS S31803 stainless steel by duplex treatment
Surface and Coatings Technology. 2010;205(5):1552-1556   Crossref logo
Link1 Link2